General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Chromium Molybdenum Steel |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Chromium Molybdenum Steel |
Tensile strength | 100.0 °C | 500 MPa Show Material materials with Tensile strength of 500 MPa | |
150.0 °C | 480 MPa Show Material materials with Tensile strength of 480 MPa | ||
200.0 °C | 460 MPa Show Material materials with Tensile strength of 460 MPa | ||
250.0 °C | 450 MPa Show Material materials with Tensile strength of 450 MPa | ||
300.0 °C | 440 MPa Show Material materials with Tensile strength of 440 MPa | ||
350.0 °C | 430 MPa Show Material materials with Tensile strength of 430 MPa | ||
400.0 °C | 410 MPa Show Material materials with Tensile strength of 410 MPa | ||
450.0 °C | 380 MPa Show Material materials with Tensile strength of 380 MPa | ||
Yield strength Rp0.2 | 100.0 °C | 338 MPa Show Material materials with Yield strength Rp0.2 of 338 MPa | |
150.0 °C | 319 MPa Show Material materials with Yield strength Rp0.2 of 319 MPa | ||
200.0 °C | 319 MPa Show Material materials with Yield strength Rp0.2 of 319 MPa | ||
250.0 °C | 309 MPa Show Material materials with Yield strength Rp0.2 of 309 MPa | ||
300.0 °C | 304 MPa Show Material materials with Yield strength Rp0.2 of 304 MPa | ||
350.0 °C | 294 MPa Show Material materials with Yield strength Rp0.2 of 294 MPa | ||
400.0 °C | 284 MPa Show Material materials with Yield strength Rp0.2 of 284 MPa | ||
450.0 °C | 275 MPa Show Material materials with Yield strength Rp0.2 of 275 MPa | ||
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.1E-5 - 1.4E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.1E-5 - 1.4E-5 1/K | Typical for Chromium Molybdenum Steel |
Melting point | 1382 - 1529 °C Show Material materials with Melting point of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel | |
Specific heat capacity | 23.0 °C | 448 - 502 J/(kg·K) Show Material materials with Specific heat capacity of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Thermal conductivity | 23.0 °C | 36 - 43 W/(m·K) Show Material materials with Thermal conductivity of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.06 - 0.15 % Show Material materials with Carbon of 0.06 - 0.15 % |
Chromium | 2.65 - 3.35 % Show Material materials with Chromium of 2.65 - 3.35 % |
Manganese | 0.3 - 0.6 % Show Material materials with Manganese of 0.3 - 0.6 % |
Molybdenum | 0.8 - 1.06 % Show Material materials with Molybdenum of 0.8 - 1.06 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.5 % Show Material materials with Silicon of 0.5 % |
Sulfur | 0.02 % Show Material materials with Sulfur of 0.02 % |
Do you have a technical question or need more information about this material?
Post it as a comment below and receive answers from engineers and other community members.