General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 8.8 g/cm³ Show Material materials with Density of 8.8 g/cm³ | Typical for Nickel Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Nickel Steel |
Elongation | 20.0 °C | 22 - 24 % Show Material materials with Elongation of 22 - 24 % | |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Nickel Steel |
Shear modulus | 23.0 °C | 76 GPa Show Material materials with Shear modulus of 76 GPa | Typical for Nickel Steel |
Tensile strength | 20.0 °C | 500 - 650 MPa Show Material materials with Tensile strength of 500 - 650 MPa | |
Yield strength | 20.0 °C | 280 - 360 MPa Show Material materials with Yield strength of 280 - 360 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Max service temperature, long | 0 - 300 °C Show Material materials with Max service temperature, long of 0 - 300 °C | ||
Melting point | 1316 - 1595 °C Show Material materials with Melting point of 1316 - 1595 °C | Typical for Nickel Steel | |
Specific heat capacity | 23.0 °C | 456 J/(kg·K) Show Material materials with Specific heat capacity of 456 J/(kg·K) | Typical for Nickel Steel |
Thermal conductivity | 23.0 °C | 10 - 50 W/(m·K) Show Material materials with Thermal conductivity of 10 - 50 W/(m·K) | Typical for Nickel Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.17 - 0.23 % Show Material materials with Carbon of 0.17 - 0.23 % |
Chromium | 0.3 % Show Material materials with Chromium of 0.3 % |
Manganese | 1 - 1.5 % Show Material materials with Manganese of 1 - 1.5 % |
Molybdenum | 0.15 % Show Material materials with Molybdenum of 0.15 % |
Nickel | 0.4 % Show Material materials with Nickel of 0.4 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 0.6 % Show Material materials with Silicon of 0.6 % |
Sulfur | 0.015 % Show Material materials with Sulfur of 0.015 % |