General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.85 g/cm³ Show Material materials with Density of 7.85 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 20.0 °C | 211 GPa Show Material materials with Elastic modulus of 211 GPa |
100.0 °C | 204 GPa Show Material materials with Elastic modulus of 204 GPa | |
200.0 °C | 196 GPa Show Material materials with Elastic modulus of 196 GPa | |
300.0 °C | 186 GPa Show Material materials with Elastic modulus of 186 GPa | |
Elongation | 20.0 °C | 10 % Show Material materials with Elongation of 10 % |
Tensile strength | 20.0 °C | 1000 - 1250 MPa Show Material materials with Tensile strength of 1000 - 1250 MPa |
Yield strength Rp0.2 | 20.0 °C | 800 - 850 MPa Show Material materials with Yield strength Rp0.2 of 800 - 850 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.1E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.1E-5 1/K |
200.0 °C | 1.2E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.2E-5 1/K | |
300.0 °C | 1.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K | |
Max service temperature, long | 0 - 300 °C Show Material materials with Max service temperature, long of 0 - 300 °C |
Chemical properties
Property | Value |
---|---|
Carbon | 0.32 - 0.39 % Show Material materials with Carbon of 0.32 - 0.39 % |
Chromium | 2.2 - 2.7 % Show Material materials with Chromium of 2.2 - 2.7 % |
Manganese | 0.6 - 1 % Show Material materials with Manganese of 0.6 - 1 % |
Molybdenum | 0.3 - 0.5 % Show Material materials with Molybdenum of 0.3 - 0.5 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 0.6 % Show Material materials with Silicon of 0.6 % |
Sulfur | 0.015 % Show Material materials with Sulfur of 0.015 % |
Vanadium | 0.05 - 0.15 % Show Material materials with Vanadium of 0.05 - 0.15 % |
Do you have a technical question or need more information about this material?
Post it as a comment below and receive answers from engineers and other community members.