General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.85 g/cm³ Show Material materials with Density of 7.85 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 211 GPa Show Material materials with Elastic modulus of 211 GPa | |
100.0 °C | 204 GPa Show Material materials with Elastic modulus of 204 GPa | ||
200.0 °C | 196 GPa Show Material materials with Elastic modulus of 196 GPa | ||
300.0 °C | 186 GPa Show Material materials with Elastic modulus of 186 GPa | ||
Elongation | 20.0 °C | 10 % Show Material materials with Elongation of 10 % | |
Poisson's ratio | 20.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Chromium Molybdenum Steel |
Tensile strength | 20.0 °C | 850 - 1100 MPa Show Material materials with Tensile strength of 850 - 1100 MPa | |
Yield strength Rp0.2 | 20.0 °C | 700 - 800 MPa Show Material materials with Yield strength Rp0.2 of 700 - 800 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.1E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.1E-5 1/K | |
200.0 °C | 1.2E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.2E-5 1/K | ||
300.0 °C | 1.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K | ||
Max service temperature, long | 0 - 300 °C Show Material materials with Max service temperature, long of 0 - 300 °C | ||
Melting point | 1382 - 1529 °C Show Material materials with Melting point of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel | |
Specific heat capacity | 20.0 °C | 448 - 502 J/(kg·K) Show Material materials with Specific heat capacity of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Thermal conductivity | 20.0 °C | 36 - 43 W/(m·K) Show Material materials with Thermal conductivity of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.38 - 0.45 % Show Material materials with Carbon of 0.38 - 0.45 % |
Chromium | 0.8 - 1.2 % Show Material materials with Chromium of 0.8 - 1.2 % |
Manganese | 0.6 - 1 % Show Material materials with Manganese of 0.6 - 1 % |
Molybdenum | 0.2 - 0.3 % Show Material materials with Molybdenum of 0.2 - 0.3 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 0.6 % Show Material materials with Silicon of 0.6 % |
Sulfur | 0.015 % Show Material materials with Sulfur of 0.015 % |