DIN 17240 Grade Ck 35 quenched and tempered (+QT)

Want to keep this datasheet? Save it now in your required format

Description

Creep resisting steel for bolts and nuts. Application temperature up to 400 °C for nuts.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.85 g/cm³

Show Material materials with Density of 7.85 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

211 GPa

Show Material materials with Elastic modulus of 211 GPa

100.0 °C

204 GPa

Show Material materials with Elastic modulus of 204 GPa

200.0 °C

196 GPa

Show Material materials with Elastic modulus of 196 GPa

300.0 °C

186 GPa

Show Material materials with Elastic modulus of 186 GPa

400.0 °C

177 GPa

Show Material materials with Elastic modulus of 177 GPa

450.0 °C

172 GPa

Show Material materials with Elastic modulus of 172 GPa

500.0 °C

164 GPa

Show Material materials with Elastic modulus of 164 GPa

550.0 °C

152 GPa

Show Material materials with Elastic modulus of 152 GPa

600.0 °C

127 GPa

Show Material materials with Elastic modulus of 127 GPa

Elongation

20.0 °C

22 %

Show Material materials with Elongation of 22 %

Poisson's ratio

23.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Medium Carbon Steel

Reduction of area

20.0 °C

45 %

Show Material materials with Reduction of area of 45 %

Shear modulus

23.0 °C

75 - 80 GPa

Show Material materials with Shear modulus of 75 - 80 GPa

Typical for Carbon Steel

Tensile strength

20.0 °C

500 - 650 MPa

Show Material materials with Tensile strength of 500 - 650 MPa

300.0 °C

400 MPa

Show Material materials with Tensile strength of 400 MPa

350.0 °C

390 MPa

Show Material materials with Tensile strength of 390 MPa

Unlock all property charts

Yield strength Rp0.2

20.0 °C

280 MPa

Show Material materials with Yield strength Rp0.2 of 280 MPa

200.0 °C

220 MPa

Show Material materials with Yield strength Rp0.2 of 220 MPa

250.0 °C

203 MPa

Show Material materials with Yield strength Rp0.2 of 203 MPa

300.0 °C

186 MPa

Show Material materials with Yield strength Rp0.2 of 186 MPa

350.0 °C

167 MPa

Show Material materials with Yield strength Rp0.2 of 167 MPa

400.0 °C

147 MPa

Show Material materials with Yield strength Rp0.2 of 147 MPa

Unlock all property charts

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

1.11E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.11E-5 1/K

200.0 °C

1.21E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.21E-5 1/K

300.0 °C

1.29E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.29E-5 1/K

400.0 °C

1.35E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.35E-5 1/K

500.0 °C

1.39E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.39E-5 1/K

600.0 °C

1.41E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.41E-5 1/K

Unlock all property charts

Max service temperature

500 °C

Show Material materials with Max service temperature of 500 °C

Typical for Carbon Steel

Max service temperature, long

0 - 350 °C

Show Material materials with Max service temperature, long of 0 - 350 °C

Melting point

1380 - 1514 °C

Show Material materials with Melting point of 1380 - 1514 °C

Typical for Medium Carbon Steel

Specific heat capacity

20.0 °C

460 J/(kg·K)

Show Material materials with Specific heat capacity of 460 J/(kg·K)

Thermal conductivity

20.0 °C

42 W/(m·K)

Show Material materials with Thermal conductivity of 42 W/(m·K)

Electrical

PropertyTemperatureValueComment

Electrical resistivity

23.0 °C

1.43E-7 - 1.74E-7 Ω·m

Show Material materials with Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m

Typical for Carbon Steel

Chemical properties

PropertyValue

Carbon

0.32 - 0.39 %

Show Material materials with Carbon of 0.32 - 0.39 %

Manganese

0.5 - 0.8 %

Show Material materials with Manganese of 0.5 - 0.8 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

0.15 - 0.35 %

Show Material materials with Silicon of 0.15 - 0.35 %

Sulfur

0.035 %

Show Material materials with Sulfur of 0.035 %