DIN 17240 Grade X22CrMoV12-1 quenched and tempered (+QT800)

View suppliers (6)
Want to keep this datasheet? Save it now in your required format

Description

Temperable high strength steel with good high temperature strength up to 580 °C and resistance to scaling up to 600 °C. Application: pressure vessel and pipeline construction, turbine construction, chemicals industry, reactor engineering, screws, nuts

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.7 - 7.76 g/cm³

Show Material materials with Density of 7.7 - 7.76 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

216 - 218 GPa

Show Material materials with Elastic modulus of 216 - 218 GPa

100.0 °C

209 - 213 GPa

Show Material materials with Elastic modulus of 209 - 213 GPa

200.0 °C

200 - 206 GPa

Show Material materials with Elastic modulus of 200 - 206 GPa

300.0 °C

190 - 198 GPa

Show Material materials with Elastic modulus of 190 - 198 GPa

400.0 °C

179 - 190 GPa

Show Material materials with Elastic modulus of 179 - 190 GPa

500.0 °C

167 - 180 GPa

Show Material materials with Elastic modulus of 167 - 180 GPa

600.0 °C

127 - 167 GPa

Show Material materials with Elastic modulus of 127 - 167 GPa

Poisson's ratio

20.0 °C

0.28 [-]

Show Material materials with Poisson's ratio of 0.28 [-]

Shear modulus

20.0 °C

84.95 GPa

Show Material materials with Shear modulus of 84.95 GPa

Yield strength Rp0.2

200.0 °C

530 MPa

Show Material materials with Yield strength Rp0.2 of 530 MPa

250.0 °C

505 MPa

Show Material materials with Yield strength Rp0.2 of 505 MPa

300.0 °C

480 MPa

Show Material materials with Yield strength Rp0.2 of 480 MPa

350.0 °C

452 MPa

Show Material materials with Yield strength Rp0.2 of 452 MPa

400.0 °C

423 MPa

Show Material materials with Yield strength Rp0.2 of 423 MPa

450.0 °C

382 MPa

Show Material materials with Yield strength Rp0.2 of 382 MPa

500.0 °C

344 MPa

Show Material materials with Yield strength Rp0.2 of 344 MPa

550.0 °C

284 MPa

Show Material materials with Yield strength Rp0.2 of 284 MPa

600.0 °C

206 MPa

Show Material materials with Yield strength Rp0.2 of 206 MPa

Unlock all property charts

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

20.0 °C

1.02E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.02E-5 1/K

100.0 °C

1.05E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.05E-5 1/K

200.0 °C

1.09E-5 - 1.1E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.09E-5 - 1.1E-5 1/K

300.0 °C

1.13E-5 - 1.15E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.13E-5 - 1.15E-5 1/K

400.0 °C

1.16E-5 - 1.2E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.16E-5 - 1.2E-5 1/K

500.0 °C

1.2E-5 - 1.23E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.2E-5 - 1.23E-5 1/K

600.0 °C

1.22E-5 - 1.25E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.22E-5 - 1.25E-5 1/K

Unlock all property charts

Max service temperature, long

0 - 580 °C

Show Material materials with Max service temperature, long of 0 - 580 °C

Melting point

1370 - 1530 °C

Show Material materials with Melting point of 1370 - 1530 °C

Typical for Martensitic Stainless Steel

Specific heat capacity

20.0 °C

439 - 460 J/(kg·K)

Show Material materials with Specific heat capacity of 439 - 460 J/(kg·K)

100.0 °C

474 J/(kg·K)

Show Material materials with Specific heat capacity of 474 J/(kg·K)

200.0 °C

498 J/(kg·K)

Show Material materials with Specific heat capacity of 498 J/(kg·K)

300.0 °C

517 J/(kg·K)

Show Material materials with Specific heat capacity of 517 J/(kg·K)

400.0 °C

538 J/(kg·K)

Show Material materials with Specific heat capacity of 538 J/(kg·K)

500.0 °C

564 J/(kg·K)

Show Material materials with Specific heat capacity of 564 J/(kg·K)

600.0 °C

598 J/(kg·K)

Show Material materials with Specific heat capacity of 598 J/(kg·K)

Unlock all property charts

Thermal conductivity

20.0 °C

24 W/(m·K)

Show Material materials with Thermal conductivity of 24 W/(m·K)

100.0 °C

24.4 - 25 W/(m·K)

Show Material materials with Thermal conductivity of 24.4 - 25 W/(m·K)

200.0 °C

24.8 - 25 W/(m·K)

Show Material materials with Thermal conductivity of 24.8 - 25 W/(m·K)

300.0 °C

25.1 - 26 W/(m·K)

Show Material materials with Thermal conductivity of 25.1 - 26 W/(m·K)

400.0 °C

25.6 - 26 W/(m·K)

Show Material materials with Thermal conductivity of 25.6 - 26 W/(m·K)

500.0 °C

26 - 26.1 W/(m·K)

Show Material materials with Thermal conductivity of 26 - 26.1 W/(m·K)

600.0 °C

26.4 - 27 W/(m·K)

Show Material materials with Thermal conductivity of 26.4 - 27 W/(m·K)

650.0 °C

29 W/(m·K)

Show Material materials with Thermal conductivity of 29 W/(m·K)

Unlock all property charts

Thermal diffusivity

20.0 °C

7.1 mm²/s

Show Material materials with Thermal diffusivity of 7.1 mm²/s

100.0 °C

6.3 mm²/s

Show Material materials with Thermal diffusivity of 6.3 mm²/s

200.0 °C

6 mm²/s

Show Material materials with Thermal diffusivity of 6 mm²/s

300.0 °C

5.7 mm²/s

Show Material materials with Thermal diffusivity of 5.7 mm²/s

400.0 °C

5.4 mm²/s

Show Material materials with Thermal diffusivity of 5.4 mm²/s

500.0 °C

4.9 mm²/s

Show Material materials with Thermal diffusivity of 4.9 mm²/s

600.0 °C

4.1 mm²/s

Show Material materials with Thermal diffusivity of 4.1 mm²/s

Unlock all property charts

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

6E-7 - 6.03E-7 Ω·m

Show Material materials with Electrical resistivity of 6E-7 - 6.03E-7 Ω·m

100.0 °C

6.68E-7 Ω·m

Show Material materials with Electrical resistivity of 6.68E-7 Ω·m

200.0 °C

7.43E-7 Ω·m

Show Material materials with Electrical resistivity of 7.43E-7 Ω·m

300.0 °C

8.17E-7 Ω·m

Show Material materials with Electrical resistivity of 8.17E-7 Ω·m

400.0 °C

8.9E-7 Ω·m

Show Material materials with Electrical resistivity of 8.9E-7 Ω·m

500.0 °C

9.62E-7 Ω·m

Show Material materials with Electrical resistivity of 9.62E-7 Ω·m

600.0 °C

1.04E-6 Ω·m

Show Material materials with Electrical resistivity of 1.04E-6 Ω·m

Unlock all property charts

Chemical properties

PropertyValue

Carbon

0.18 - 0.24 %

Show Material materials with Carbon of 0.18 - 0.24 %

Chromium

11 - 12.5 %

Show Material materials with Chromium of 11 - 12.5 %

Manganese

0.3 - 0.8 %

Show Material materials with Manganese of 0.3 - 0.8 %

Molybdenum

0.8 - 1.2 %

Show Material materials with Molybdenum of 0.8 - 1.2 %

Nickel

0.3 - 0.8 %

Show Material materials with Nickel of 0.3 - 0.8 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

0.1 - 0.5 %

Show Material materials with Silicon of 0.1 - 0.5 %

Sulfur

0.035 %

Show Material materials with Sulfur of 0.035 %

Vanadium

0.25 - 0.35 %

Show Material materials with Vanadium of 0.25 - 0.35 %

Do you have a technical question or need more information about this material?

Post it as a comment below and receive answers from engineers and other community members.