DIN 17465 Grade GX40CrSi17 soft annealed (+A)

Want to keep this datasheet? Save it now in your required format

Description

G-X 40 CrSi 17, basically for parts of oven for medium mechanical loadings, like widdle grate, rods for grates, pipe clamp and pipe connexion, distance plates, far jet nozzles. In cement industry for protecting rings and protecting archs, segments etc., for cased insert box and attachments for superheater. resistance: - in oxidising burning atmosphere: 950°C - in reductive burning atmosphere: 900°C - in oxidising sulfureous gas: 950°C - in reductive sulfureous gas: 900°C

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.7 g/cm³

Show Material materials with Density of 7.7 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

220 GPa

Show Material materials with Elastic modulus of 220 GPa

Typical for Ferritic Stainless Steel

Hardness, Brinell

20.0 °C

300 [-]

Show Material materials with Hardness, Brinell of 300 [-]

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Ferritic Stainless Steel

Shear modulus

23.0 °C

77 GPa

Show Material materials with Shear modulus of 77 GPa

Typical for Ferritic Stainless Steel

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

400.0 °C

1.25E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.25E-5 1/K

800.0 °C

1.35E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.35E-5 1/K

Max service temperature, long

0 - 950 °C

Show Material materials with Max service temperature, long of 0 - 950 °C

Melting point

1425 - 1530 °C

Show Material materials with Melting point of 1425 - 1530 °C

Typical for Ferritic Stainless Steel

Specific heat capacity

20.0 °C

500 J/(kg·K)

Show Material materials with Specific heat capacity of 500 J/(kg·K)

Thermal conductivity

20.0 °C

18.8 W/(m·K)

Show Material materials with Thermal conductivity of 18.8 W/(m·K)

Electrical

PropertyTemperatureValueComment

Electrical resistivity

23.0 °C

6E-7 - 7.5E-7 Ω·m

Show Material materials with Electrical resistivity of 6E-7 - 7.5E-7 Ω·m

Typical for Ferritic Stainless Steel

Chemical properties

PropertyValue

Carbon

0.3 - 0.45 %

Show Material materials with Carbon of 0.3 - 0.45 %

Chromium

16 - 18 %

Show Material materials with Chromium of 16 - 18 %

Manganese

0.5 - 1 %

Show Material materials with Manganese of 0.5 - 1 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

1 - 2.5 %

Show Material materials with Silicon of 1 - 2.5 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %

Do you have a technical question or need more information about this material?