General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation | 20.0 °C | 14 % Show Material materials with Elongation of 14 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Tensile strength | 20.0 °C | 790 - 940 MPa Show Material materials with Tensile strength of 790 - 940 MPa | |
Yield strength | 20.0 °C | 690 MPa Show Material materials with Yield strength of 690 MPa |
Thermal
Property | Value |
---|---|
Max service temperature, long | -60 - 0 °C Show Material materials with Max service temperature, long of -60 - 0 °C |
Chemical properties
Property | Value |
---|---|
Carbon | 0.2 % Show Material materials with Carbon of 0.2 % |
Chromium | 0.5 - 1 % Show Material materials with Chromium of 0.5 - 1 % |
Manganese | 0.7 - 1.2 % Show Material materials with Manganese of 0.7 - 1.2 % |
Molybdenum | 0.2 - 0.6 % Show Material materials with Molybdenum of 0.2 - 0.6 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 0.4 - 0.8 % Show Material materials with Silicon of 0.4 - 0.8 % |
Sulfur | 0.01 % Show Material materials with Sulfur of 0.01 % |
Zirconium | 0.12 % Show Material materials with Zirconium of 0.12 % |