General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.9 g/cm³ Show Material materials with Density of 7.9 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 195 GPa Show Material materials with Elastic modulus of 195 GPa | Typical for Austenitic Stainless Steel |
Elongation | 20.0 °C | 20 % Show Material materials with Elongation of 20 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Austenitic Stainless Steel |
Shear modulus | 23.0 °C | 77 GPa Show Material materials with Shear modulus of 77 GPa | Typical for Austenitic Stainless Steel |
Tensile strength | 20.0 °C | 440 - 590 MPa Show Material materials with Tensile strength of 440 - 590 MPa | |
Yield strength Rp0.2 | 20.0 °C | 195 MPa Show Material materials with Yield strength Rp0.2 of 195 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.65E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.65E-5 1/K | |
200.0 °C | 1.75E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.75E-5 1/K | ||
300.0 °C | 1.75E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.75E-5 1/K | ||
Melting point | 1230 - 1480 °C Show Material materials with Melting point of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Specific heat capacity | 23.0 °C | 440 J/(kg·K) Show Material materials with Specific heat capacity of 440 J/(kg·K) | Typical for Austenitic Stainless Steel |
Thermal conductivity | 20.0 °C | 15 W/(m·K) Show Material materials with Thermal conductivity of 15 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 20.0 °C | 7.3E-7 Ω·m Show Material materials with Electrical resistivity of 7.3E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Carbon | 0.15 % Show Material materials with Carbon of 0.15 % |
Chromium | 16.5 - 18.5 % Show Material materials with Chromium of 16.5 - 18.5 % |
Manganese | 2 % Show Material materials with Manganese of 2 % |
Molybdenum | 0.75 % Show Material materials with Molybdenum of 0.75 % |
Nickel | 10 - 12 % Show Material materials with Nickel of 10 - 12 % |
Phosphorus | 0.05 % Show Material materials with Phosphorus of 0.05 % |
Silicon | 1 % Show Material materials with Silicon of 1 % |
Sulfur | 0.03 % Show Material materials with Sulfur of 0.03 % |