SEW 395 Grade GX2CrNiMoN18-14 solution heat-treated and quenched

Want to keep this datasheet? Save it now in your required format

Description

The fully austenitic material GX2CrNiMoN18-14, with the material number 1.3960 according to SEW 395-98 (the former G-X 2 CrNiMoN 18 14, material number 1.3952 according to SEW 395-87), possesses a defined low value of the relative magnetic permeability of 1.01 maximum (for castings with a wall thickness of up to 50 mm). It is applied for construction components which an interference or shielding of a magnetic field must not occur at. (SEW: steel-iron material specification)

Related Standards

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

195 GPa

Show Material materials with Elastic modulus of 195 GPa

Typical for Austenitic Stainless Steel

Elongation

20.0 °C

30 %

Show Material materials with Elongation of 30 %

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Austenitic Stainless Steel

Shear modulus

23.0 °C

77 GPa

Show Material materials with Shear modulus of 77 GPa

Typical for Austenitic Stainless Steel

Tensile strength

20.0 °C

490 - 690 MPa

Show Material materials with Tensile strength of 490 - 690 MPa

Yield strength Rp0.2

20.0 °C

240 MPa

Show Material materials with Yield strength Rp0.2 of 240 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

1.65E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.65E-5 1/K

200.0 °C

1.75E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.75E-5 1/K

300.0 °C

1.75E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.75E-5 1/K

Melting point

1230 - 1480 °C

Show Material materials with Melting point of 1230 - 1480 °C

Typical for Austenitic Stainless Steel

Specific heat capacity

23.0 °C

440 J/(kg·K)

Show Material materials with Specific heat capacity of 440 J/(kg·K)

Typical for Austenitic Stainless Steel

Thermal conductivity

20.0 °C

15 W/(m·K)

Show Material materials with Thermal conductivity of 15 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

7.5E-7 Ω·m

Show Material materials with Electrical resistivity of 7.5E-7 Ω·m

Chemical properties

PropertyValue

Carbon

0.03 %

Show Material materials with Carbon of 0.03 %

Chromium

16.5 - 18.5 %

Show Material materials with Chromium of 16.5 - 18.5 %

Manganese

2 %

Show Material materials with Manganese of 2 %

Molybdenum

2.5 - 3 %

Show Material materials with Molybdenum of 2.5 - 3 %

Nickel

13 - 15 %

Show Material materials with Nickel of 13 - 15 %

Nitrogen

0.15 - 0.25 %

Show Material materials with Nitrogen of 0.15 - 0.25 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Sulfur

0.02 %

Show Material materials with Sulfur of 0.02 %