General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 200 GPa Show Material materials with Elastic modulus of 200 GPa | Typical for Duplex Stainless Steel |
Elongation | 20.0 °C | 22 % Show Material materials with Elongation of 22 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Duplex Stainless Steel |
Shear modulus | 23.0 °C | 77 GPa Show Material materials with Shear modulus of 77 GPa | Typical for Duplex Stainless Steel |
Tensile strength | 20.0 °C | 650 - 850 MPa Show Material materials with Tensile strength of 650 - 850 MPa | |
Yield strength Rp0.2 | 20.0 °C | 480 MPa Show Material materials with Yield strength Rp0.2 of 480 MPa | |
100.0 °C | 390 MPa Show Material materials with Yield strength Rp0.2 of 390 MPa | ||
200.0 °C | 330 MPa Show Material materials with Yield strength Rp0.2 of 330 MPa | ||
300.0 °C | 295 MPa Show Material materials with Yield strength Rp0.2 of 295 MPa | ||
350.0 °C | 280 MPa Show Material materials with Yield strength Rp0.2 of 280 MPa | ||
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.4E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.4E-5 1/K | |
200.0 °C | 1.45E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.45E-5 1/K | ||
300.0 °C | 1.49E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.49E-5 1/K | ||
Max service temperature | 300 °C Show Material materials with Max service temperature of 300 °C | Typical for Duplex Stainless Steel | |
Max service temperature, long | 0 - 300 °C Show Material materials with Max service temperature, long of 0 - 300 °C | ||
Melting point | 1375 - 1450 °C Show Material materials with Melting point of 1375 - 1450 °C | Typical for Duplex Stainless Steel | |
Specific heat capacity | 20.0 °C | 450 J/(kg·K) Show Material materials with Specific heat capacity of 450 J/(kg·K) | |
Thermal conductivity | 20.0 °C | 15 W/(m·K) Show Material materials with Thermal conductivity of 15 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbon | 0.03 % Show Material materials with Carbon of 0.03 % |
Chromium | 24.5 - 26.5 % Show Material materials with Chromium of 24.5 - 26.5 % |
Copper | 2.75 - 3.5 % Show Material materials with Copper of 2.75 - 3.5 % |
Manganese | 2 % Show Material materials with Manganese of 2 % |
Molybdenum | 2.5 - 3.5 % Show Material materials with Molybdenum of 2.5 - 3.5 % |
Nickel | 5 - 7 % Show Material materials with Nickel of 5 - 7 % |
Nitrogen | 0.12 - 0.25 % Show Material materials with Nitrogen of 0.12 - 0.25 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 1 % Show Material materials with Silicon of 1 % |
Sulfur | 0.02 % Show Material materials with Sulfur of 0.02 % |