General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.9 g/cm³ Show Material materials with Density of 7.9 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elongation | 20.0 °C | 20 % Show Material materials with Elongation of 20 % |
Tensile strength | 20.0 °C | 570 - 800 MPa Show Material materials with Tensile strength of 570 - 800 MPa |
Yield strength Rp0.2 | 20.0 °C | 315 MPa Show Material materials with Yield strength Rp0.2 of 315 MPa |
100.0 °C | 220 MPa Show Material materials with Yield strength Rp0.2 of 220 MPa | |
200.0 °C | 170 MPa Show Material materials with Yield strength Rp0.2 of 170 MPa | |
300.0 °C | 140 MPa Show Material materials with Yield strength Rp0.2 of 140 MPa | |
350.0 °C | 130 MPa Show Material materials with Yield strength Rp0.2 of 130 MPa | |
400.0 °C | 120 MPa Show Material materials with Yield strength Rp0.2 of 120 MPa | |
Yield strength Rp1.0 | 20.0 °C | 340 MPa Show Material materials with Yield strength Rp1.0 of 340 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.57E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.57E-5 1/K |
200.0 °C | 1.7E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.7E-5 1/K | |
300.0 °C | 1.75E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.75E-5 1/K | |
Specific heat capacity | 20.0 °C | 500 J/(kg·K) Show Material materials with Specific heat capacity of 500 J/(kg·K) |
Thermal conductivity | 20.0 °C | 14 W/(m·K) Show Material materials with Thermal conductivity of 14 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbon | 0.03 % Show Material materials with Carbon of 0.03 % |
Chromium | 20 - 22 % Show Material materials with Chromium of 20 - 22 % |
Manganese | 3 - 6 % Show Material materials with Manganese of 3 - 6 % |
Molybdenum | 3 - 3.5 % Show Material materials with Molybdenum of 3 - 3.5 % |
Nickel | 14 - 17 % Show Material materials with Nickel of 14 - 17 % |
Niobium | 0.25 % Show Material materials with Niobium of 0.25 % |
Nitrogen | 0.2 - 0.35 % Show Material materials with Nitrogen of 0.2 - 0.35 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 1 % Show Material materials with Silicon of 1 % |
Sulfur | 0.01 % Show Material materials with Sulfur of 0.01 % |