General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Nickel Chromium Molybdenum Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Nickel Chromium Molybdenum Steel |
Elongation | 20.0 °C | 16 % Show Material materials with Elongation of 16 % | |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Nickel Chromium Molybdenum Steel |
Tensile strength | 20.0 °C | 650 - 800 MPa Show Material materials with Tensile strength of 650 - 800 MPa | |
Yield strength | 20.0 °C | 550 MPa Show Material materials with Yield strength of 550 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | -196.0 °C | 8.6E-6 1/K Show Material materials with Coefficient of thermal expansion of 8.6E-6 1/K | |
-170.0 °C | 9.4E-6 1/K Show Material materials with Coefficient of thermal expansion of 9.4E-6 1/K | ||
-120.0 °C | 1.03E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.03E-5 1/K | ||
-50.0 °C | 1.12E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.12E-5 1/K | ||
-25.0 °C | 1.14E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.14E-5 1/K | ||
Melting point | 1382 - 1529 °C Show Material materials with Melting point of 1382 - 1529 °C | Typical for Nickel Chromium Molybdenum Steel | |
Specific heat capacity | 23.0 °C | 448 - 670 J/(kg·K) Show Material materials with Specific heat capacity of 448 - 670 J/(kg·K) | Typical for Nickel Chromium Molybdenum Steel |
Thermal conductivity | -20.0 °C | 35 W/(m·K) Show Material materials with Thermal conductivity of 35 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbon | 0.12 - 0.16 % Show Material materials with Carbon of 0.12 - 0.16 % |
Chromium | 1.3 - 1.8 % Show Material materials with Chromium of 1.3 - 1.8 % |
Manganese | 0.55 - 0.7 % Show Material materials with Manganese of 0.55 - 0.7 % |
Molybdenum | 0.45 - 0.55 % Show Material materials with Molybdenum of 0.45 - 0.55 % |
Nickel | 2.7 - 3 % Show Material materials with Nickel of 2.7 - 3 % |
Phosphorus | 0.01 % Show Material materials with Phosphorus of 0.01 % |
Silicon | 0.3 % Show Material materials with Silicon of 0.3 % |
Sulfur | 0.01 % Show Material materials with Sulfur of 0.01 % |