General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.7 g/cm³ Show Material materials with Density of 7.7 g/cm³ |
Material Information
Property | Value |
---|---|
Dimension | 0.0-300.0 |
Mechanical
Property | Temperature | Value |
---|---|---|
Elongation | 20.0 °C | 0 - 15 % Show Material materials with Elongation of 0 - 15 % |
Tensile strength | 20.0 °C | 720 - 900 MPa Show Material materials with Tensile strength of 720 - 900 MPa |
Yield strength | 20.0 °C | 0 - 520 MPa Show Material materials with Yield strength of 0 - 520 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | -195.0 °C | 8.6E-6 1/K Show Material materials with Coefficient of thermal expansion of 8.6E-6 1/K |
-170.0 °C | 9.3E-6 1/K Show Material materials with Coefficient of thermal expansion of 9.3E-6 1/K | |
-120.0 °C | 1.01E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.01E-5 1/K | |
-50.0 °C | 1.08E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.08E-5 1/K | |
-25.0 °C | 1.1E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.1E-5 1/K | |
Max service temperature, long | -120 °C Show Material materials with Max service temperature, long of -120 °C | |
Thermal conductivity | -20.0 °C | 30 W/(m·K) Show Material materials with Thermal conductivity of 30 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbon | 0.05 % Show Material materials with Carbon of 0.05 % |
Chromium | 12 - 13.5 % Show Material materials with Chromium of 12 - 13.5 % |
Manganese | 1.5 % Show Material materials with Manganese of 1.5 % |
Molybdenum | 0.4 - 0.7 % Show Material materials with Molybdenum of 0.4 - 0.7 % |
Nickel | 3.5 - 5 % Show Material materials with Nickel of 3.5 - 5 % |
Phosphorus | 0.04 % Show Material materials with Phosphorus of 0.04 % |
Silicon | 0.8 % Show Material materials with Silicon of 0.8 % |
Sulfur | 0.015 % Show Material materials with Sulfur of 0.015 % |