General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.85 g/cm³ Show Material materials with Density of 7.85 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation | 20.0 °C | 11 % Show Material materials with Elongation of 11 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Tensile strength | 20.0 °C | 736 MPa Show Material materials with Tensile strength of 736 MPa | |
Yield strength | 20.0 °C | 520 MPa Show Material materials with Yield strength of 520 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.46 - 0.54 % Show Material materials with Carbon of 0.46 - 0.54 % |
Chromium | 0.9 - 1.2 % Show Material materials with Chromium of 0.9 - 1.2 % |
Manganese | 0.5 - 0.8 % Show Material materials with Manganese of 0.5 - 0.8 % |
Phosphorus | 0.04 % Show Material materials with Phosphorus of 0.04 % |
Silicon | 0.25 - 0.5 % Show Material materials with Silicon of 0.25 - 0.5 % |
Sulfur | 0.035 % Show Material materials with Sulfur of 0.035 % |
Vanadium | 0.07 - 0.12 % Show Material materials with Vanadium of 0.07 - 0.12 % |