EN 10209 Grade DC04ED cold rolled, skin passed

Want to keep this datasheet? Save it now in your required format

Description

Cold rolled low carbon steel for flat products for vitreous enamelling (direct enamelling, as well as for special applications of conventional two coat enamelling for better sag resistance). Application: domestic appliances (cooking, laundry), sanitary ware (bathtubs, shower trays, sinks), architectural panels (interior and exterior), signage,The soft unalloyed steel DCO4ED, mat. No. 1.0394, is a cold formable steel and suitable for direct enameling as well as for special conventional applications of two-coat enameling, especially if there is a need for preferably non deforming enameling. In this case are necessary special measures in order to improve enamel`s adhesion. Mechanical specific values and freedom of stretcher strains are warranted for 6 months. Application: construction components of increased deformation requirements pots, pans, covering caps for gas kitchen stoves, baking sheets, simple shower bases etc. Welding: DC04ED is weldable acc. to the fusion welding methods: MAG (metal active gas/plasma welding arc hand welding laser welding gas welding resistance welding (spot, roll seam, buckle welding)

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

20.0 °C

7.8 - 7.9 g/cm³

Show Material materials with Density of 7.8 - 7.9 g/cm³

Typical for Low Carbon Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

200 - 215 GPa

Show Material materials with Elastic modulus of 200 - 215 GPa

Typical for Low Carbon Steel

Elongation A80

20.0 °C

38 %

Show Material materials with Elongation A80 of 38 %

Elongation A80, transverse

20.0 °C

34 - 38 %

Show Material materials with Elongation A80, transverse of 34 - 38 %

Poisson's ratio

20.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Low Carbon Steel

Tensile strength

20.0 °C

270 - 350 MPa

Show Material materials with Tensile strength of 270 - 350 MPa

Tensile strength, transverse

20.0 °C

270 - 350 MPa

Show Material materials with Tensile strength, transverse of 270 - 350 MPa

Yield strength

20.0 °C

140 - 210 MPa

Show Material materials with Yield strength of 140 - 210 MPa

Yield strength, transverse

20.0 °C

140 - 260 MPa

Show Material materials with Yield strength, transverse of 140 - 260 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

20.0 °C

1.32E-5 - 1.38E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.32E-5 - 1.38E-5 1/K

Typical for Low Carbon Steel

Melting point

1480 - 1526 °C

Show Material materials with Melting point of 1480 - 1526 °C

Typical for Low Carbon Steel

Magnetic

PropertyValueComment

Curie temperature

770 °C

Show Material materials with Curie temperature of 770 °C

Typical for Low Carbon Steel

Chemical properties

PropertyValue

Carbon

4E-3 %

Show Material materials with Carbon of 4E-3 %

Manganese

0.4 %

Show Material materials with Manganese of 0.4 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Sulfur

0.05 %

Show Material materials with Sulfur of 0.05 %