EN 10089 Grade 50SiCrMo6 quenched and tempered (+QT)

Want to keep this datasheet? Save it now in your required format

Description

The steel 50SiCrMo6 is used for hot formed springs for high stress in the vehicle engineering.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Typical for Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

190 - 210 GPa

Show Material materials with Elastic modulus of 190 - 210 GPa

Typical for Steel

Elongation

20.0 °C

6 %

Show Material materials with Elongation of 6 %

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Reduction of area

20.0 °C

30 %

Show Material materials with Reduction of area of 30 %

Tensile strength

20.0 °C

1650 - 1950 MPa

Show Material materials with Tensile strength of 1650 - 1950 MPa

Yield strength Rp0.2

20.0 °C

1420 MPa

Show Material materials with Yield strength Rp0.2 of 1420 MPa

Chemical properties

PropertyValue

Carbon

0.46 - 0.54 %

Show Material materials with Carbon of 0.46 - 0.54 %

Chromium

0.8 - 1.1 %

Show Material materials with Chromium of 0.8 - 1.1 %

Manganese

0.7 - 1 %

Show Material materials with Manganese of 0.7 - 1 %

Molybdenum

0.2 - 0.35 %

Show Material materials with Molybdenum of 0.2 - 0.35 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

1.4 - 1.8 %

Show Material materials with Silicon of 1.4 - 1.8 %

Sulfur

0.025 %

Show Material materials with Sulfur of 0.025 %

Technological properties

Property
Features

Spring