EN 10213 Grade GP280GH normalized or normalized formed (+N)

Want to keep this datasheet? Save it now in your required format

Description

Material GP280GH is applicated at room temperature and increased temperatures.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

200 - 215 GPa

Show Material materials with Elastic modulus of 200 - 215 GPa

Typical for High Carbon Steel

Elongation

20.0 °C

22 %

Show Material materials with Elongation of 22 %

Poisson's ratio

23.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for High Carbon Steel

Shear modulus

23.0 °C

81 GPa

Show Material materials with Shear modulus of 81 GPa

Typical for High Carbon Steel

Tensile strength

20.0 °C

480 - 640 MPa

Show Material materials with Tensile strength of 480 - 640 MPa

Yield strength Rp0.2

20.0 °C

280 MPa

Show Material materials with Yield strength Rp0.2 of 280 MPa

100.0 °C

250 MPa

Show Material materials with Yield strength Rp0.2 of 250 MPa

200.0 °C

220 MPa

Show Material materials with Yield strength Rp0.2 of 220 MPa

300.0 °C

190 MPa

Show Material materials with Yield strength Rp0.2 of 190 MPa

350.0 °C

170 MPa

Show Material materials with Yield strength Rp0.2 of 170 MPa

400.0 °C

160 MPa

Show Material materials with Yield strength Rp0.2 of 160 MPa

450.0 °C

150 MPa

Show Material materials with Yield strength Rp0.2 of 150 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

1.28E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.28E-5 1/K

300.0 °C

1.36E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.36E-5 1/K

500.0 °C

1.45E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.45E-5 1/K

Unlock all property charts

Max service temperature

500 °C

Show Material materials with Max service temperature of 500 °C

Typical for Carbon Steel

Melting point

1289 - 1478 °C

Show Material materials with Melting point of 1289 - 1478 °C

Typical for High Carbon Steel

Specific heat capacity

20.0 °C

460 J/(kg·K)

Show Material materials with Specific heat capacity of 460 J/(kg·K)

Thermal conductivity

50.0 °C

45 W/(m·K)

Show Material materials with Thermal conductivity of 45 W/(m·K)

Electrical

PropertyTemperatureValueComment

Electrical resistivity

23.0 °C

1.43E-7 - 1.74E-7 Ω·m

Show Material materials with Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m

Typical for Carbon Steel

Chemical properties

PropertyValue

Carbon

0.18 - 0.25 %

Show Material materials with Carbon of 0.18 - 0.25 %

Chromium

0.3 %

Show Material materials with Chromium of 0.3 %

Copper

0.3 %

Show Material materials with Copper of 0.3 %

Manganese

0.8 - 1.2 %

Show Material materials with Manganese of 0.8 - 1.2 %

Molybdenum

0.12 %

Show Material materials with Molybdenum of 0.12 %

Nickel

0.4 %

Show Material materials with Nickel of 0.4 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.6 %

Show Material materials with Silicon of 0.6 %

Sulfur

0.02 %

Show Material materials with Sulfur of 0.02 %

Vanadium

0.03 %

Show Material materials with Vanadium of 0.03 %