EN 10213 Grade G17CrMoV5-10 quenched and tempered (+QT)

Want to keep this datasheet? Save it now in your required format

Description

Elevated temperature resistant steel casting for pressure purposes, e.g. turbines and steam boilers.

Related Standards

Equivalent Materials

Ashby charts

See where EN 10213 Grade G17CrMoV5-10 quenched and tempered (+QT) falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

7.85 g/cm³ at 20 °C

Mechanical

Elastic modulus

E

211 GPa at 20 °C

Show Chromium Molybdenum Steel materials with Elastic modulus of 211 GPa at 20 °C

Hide chart

Elongation

A

15 % at 20 °C

Show Chromium Molybdenum Steel materials with Elongation of 15 % at 20 °C

Poisson's ratio

ν

0.29 [-] at 23 °C

Show Chromium Molybdenum Steel materials with Poisson's ratio of 0.29 [-] at 23 °C

Typical for Chromium Molybdenum Steel

Tensile strength

Rm

590 - 780 MPa at 20 °C

Show Chromium Molybdenum Steel materials with Tensile strength of 590 - 780 MPa at 20 °C

Yield strength Rp0.2

Rp0.2

440 MPa at 20 °C

Show Chromium Molybdenum Steel materials with Yield strength Rp0.2 of 440 MPa at 20 °C

Unlock all property charts

Yield strength Rp1.0

Rp1.0

200 MPa at 20 °C

Show Chromium Molybdenum Steel materials with Yield strength Rp1.0 of 200 MPa at 20 °C

Thermal

Coefficient of thermal expansion

α

1.24E-5 1/K at 100 °C

Unlock all property charts

Max service temperature, long

Tmaxlong

300 - 610 °C

Melting point

Tm

1382 - 1529 °C

Typical for Chromium Molybdenum Steel

Specific heat capacity

cp

460 J/(kg·K) at 20 °C

Thermal conductivity

λ

50 W/(m·K) at 20 °C

Unlock all property charts

Electrical

Electrical resistivity

ρel

1.6E-7 Ω·m at 20 °C

Chemical properties

Element

Weight %

Comment

Cr

1.2 - 1.5 %

Mo

0.9 - 1.1 %

Si

0.6 %

Mn

0.5 - 0.9 %

Ni

0.4 %

More

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.