EN 10213 Grade G12MoCrV5-2 quenched and tempered (+QT)

Want to keep this datasheet? Save it now in your required format

Description

Material G12MoCrV5-2 is used at room temperature and increased temperatures in pressure vessel construction.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.85 g/cm³

Show Material materials with Density of 7.85 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

200 - 215 GPa

Show Material materials with Elastic modulus of 200 - 215 GPa

Typical for Chromium Molybdenum Steel

Elongation

20.0 °C

17 %

Show Material materials with Elongation of 17 %

Poisson's ratio

23.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Chromium Molybdenum Steel

Tensile strength

20.0 °C

510 - 660 MPa

Show Material materials with Tensile strength of 510 - 660 MPa

Yield strength Rp0.2

20.0 °C

295 MPa

Show Material materials with Yield strength Rp0.2 of 295 MPa

100.0 °C

264 MPa

Show Material materials with Yield strength Rp0.2 of 264 MPa

200.0 °C

244 MPa

Show Material materials with Yield strength Rp0.2 of 244 MPa

300.0 °C

230 MPa

Show Material materials with Yield strength Rp0.2 of 230 MPa

400.0 °C

214 MPa

Show Material materials with Yield strength Rp0.2 of 214 MPa

500.0 °C

194 MPa

Show Material materials with Yield strength Rp0.2 of 194 MPa

550.0 °C

144 MPa

Show Material materials with Yield strength Rp0.2 of 144 MPa

Yield strength Rp1.0

20.0 °C

200 MPa

Show Material materials with Yield strength Rp1.0 of 200 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.1E-5 - 1.4E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.1E-5 - 1.4E-5 1/K

Typical for Chromium Molybdenum Steel

Melting point

1382 - 1529 °C

Show Material materials with Melting point of 1382 - 1529 °C

Typical for Chromium Molybdenum Steel

Specific heat capacity

20.0 °C

460 J/(kg·K)

Show Material materials with Specific heat capacity of 460 J/(kg·K)

Thermal conductivity

23.0 °C

36 - 43 W/(m·K)

Show Material materials with Thermal conductivity of 36 - 43 W/(m·K)

Typical for Chromium Molybdenum Steel

Chemical properties

PropertyValue

Carbon

0.1 - 0.15 %

Show Material materials with Carbon of 0.1 - 0.15 %

Chromium

0.3 - 0.5 %

Show Material materials with Chromium of 0.3 - 0.5 %

Copper

0.3 %

Show Material materials with Copper of 0.3 %

Manganese

0.4 - 0.7 %

Show Material materials with Manganese of 0.4 - 0.7 %

Molybdenum

0.4 - 0.6 %

Show Material materials with Molybdenum of 0.4 - 0.6 %

Nickel

0.4 %

Show Material materials with Nickel of 0.4 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.45 %

Show Material materials with Silicon of 0.45 %

Sulfur

0.02 %

Show Material materials with Sulfur of 0.02 %

Tin

0.03 %

Show Material materials with Tin of 0.03 %

Vanadium

0.22 - 0.3 %

Show Material materials with Vanadium of 0.22 - 0.3 %