Tough at low temperature steel casting for pressure purposes, e.g. for refrigerating plants and fittings.
See where EN 10213 Grade G9Ni14 quenched and tempered (+QT) falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ7.85 g/cm³ at 20 °C
Coefficient of thermal expansion
α8.5E-6 1/K at -195 °C
Max service temperature, long
Tmaxlong-90 - 0 °C
Melting point
Tm1316 - 1595 °C
Typical for Nickel Steel
Specific heat capacity
cp460 J/(kg·K) at 20 °C
Thermal conductivity
λ35 W/(m·K) at -20 °C
Element
Weight %
Comment
3 - 4 %
0.6 %
0.5 - 0.8 %
0.3 %
0.3 %