Description

Tubes made from cryogenic unalloyed quality steel P215NL are predominantly used in apparatus, tank, line construction as well as in general machine and equipment engineering. Weldability is available.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.8 - 7.9 g/cm³

Show Material materials with Density of 7.8 - 7.9 g/cm³

Typical for Low Carbon Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

200 - 215 GPa

Show Material materials with Elastic modulus of 200 - 215 GPa

Typical for Low Carbon Steel

Elongation

20.0 °C

25 %

Show Material materials with Elongation of 25 %

Elongation, transverse

20.0 °C

23 %

Show Material materials with Elongation, transverse of 23 %

Poisson's ratio

23.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Low Carbon Steel

Shear modulus

23.0 °C

82 GPa

Show Material materials with Shear modulus of 82 GPa

Typical for Low Carbon Steel

Tensile strength

20.0 °C

360 - 480 MPa

Show Material materials with Tensile strength of 360 - 480 MPa

Tensile strength, transverse

20.0 °C

360 - 480 MPa

Show Material materials with Tensile strength, transverse of 360 - 480 MPa

Yield strength Rp0.2

20.0 °C

215 MPa

Show Material materials with Yield strength Rp0.2 of 215 MPa

100.0 °C

175 MPa

Show Material materials with Yield strength Rp0.2 of 175 MPa

200.0 °C

145 MPa

Show Material materials with Yield strength Rp0.2 of 145 MPa

250.0 °C

130 MPa

Show Material materials with Yield strength Rp0.2 of 130 MPa

300.0 °C

115 MPa

Show Material materials with Yield strength Rp0.2 of 115 MPa

Yield strength Rp0.2, transverse

20.0 °C

215 MPa

Show Material materials with Yield strength Rp0.2, transverse of 215 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.32E-5 - 1.38E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.32E-5 - 1.38E-5 1/K

Typical for Low Carbon Steel

Max service temperature

500 °C

Show Material materials with Max service temperature of 500 °C

Typical for Carbon Steel

Melting point

1480 - 1526 °C

Show Material materials with Melting point of 1480 - 1526 °C

Typical for Low Carbon Steel

Specific heat capacity

23.0 °C

465 J/(kg·K)

Show Material materials with Specific heat capacity of 465 J/(kg·K)

Typical for Low Carbon Steel

Thermal conductivity

23.0 °C

25 - 93 W/(m·K)

Show Material materials with Thermal conductivity of 25 - 93 W/(m·K)

Typical for Low Carbon Steel

Electrical

PropertyTemperatureValueComment

Electrical resistivity

23.0 °C

1.43E-7 - 1.74E-7 Ω·m

Show Material materials with Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m

Typical for Carbon Steel

Magnetic

PropertyValueComment

Curie temperature

770 °C

Show Material materials with Curie temperature of 770 °C

Typical for Low Carbon Steel

Chemical properties

PropertyValue

Aluminium

0.02 %

Show Material materials with Aluminium of 0.02 %

Carbon

0.15 %

Show Material materials with Carbon of 0.15 %

Chromium

0.3 %

Show Material materials with Chromium of 0.3 %

Copper

0.3 %

Show Material materials with Copper of 0.3 %

Manganese

0.4 - 1.2 %

Show Material materials with Manganese of 0.4 - 1.2 %

Molybdenum

0.08 %

Show Material materials with Molybdenum of 0.08 %

Nickel

0.3 %

Show Material materials with Nickel of 0.3 %

Niobium

0.01 %

Show Material materials with Niobium of 0.01 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.35 %

Show Material materials with Silicon of 0.35 %

Sulfur

0.01 - 0.02 %

Show Material materials with Sulfur of 0.01 - 0.02 %

Titanium

0.04 %

Show Material materials with Titanium of 0.04 %

Vanadium

0.02 %

Show Material materials with Vanadium of 0.02 %