EN 10216-4 Grade X12Ni5 normalized and tempered (+NT)

Want to keep this datasheet? Save it now in your required format

Description

Tubes made from cryogenic alloyed high-grade steel X12Ni5 are predominantly used in apparatus, tank, line construction as well as in general machine and equipment engineering. Weldability is available.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.86 g/cm³

Show Material materials with Density of 7.86 g/cm³

27.0 °C

7.82 g/cm³

Show Material materials with Density of 7.82 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

-269.0 °C

209.4 GPa

Show Material materials with Elastic modulus of 209.4 GPa

-200.0 °C

209.5 GPa

Show Material materials with Elastic modulus of 209.5 GPa

-150.0 °C

208 GPa

Show Material materials with Elastic modulus of 208 GPa

-100.0 °C

205.9 - 210 GPa

Show Material materials with Elastic modulus of 205.9 - 210 GPa

-50.0 °C

203.1 GPa

Show Material materials with Elastic modulus of 203.1 GPa

20.0 °C

204 GPa

Show Material materials with Elastic modulus of 204 GPa

27.0 °C

198.4 GPa

Show Material materials with Elastic modulus of 198.4 GPa

100.0 °C

199 GPa

Show Material materials with Elastic modulus of 199 GPa

200.0 °C

193 GPa

Show Material materials with Elastic modulus of 193 GPa

300.0 °C

186 GPa

Show Material materials with Elastic modulus of 186 GPa

400.0 °C

178 GPa

Show Material materials with Elastic modulus of 178 GPa

Unlock all property charts

Elongation

20.0 °C

21 %

Show Material materials with Elongation of 21 %

Elongation, transverse

20.0 °C

19 %

Show Material materials with Elongation, transverse of 19 %

Poisson's ratio

-269.0 °C

0.28 [-]

Show Material materials with Poisson's ratio of 0.28 [-]

-200.0 °C

0.28 [-]

Show Material materials with Poisson's ratio of 0.28 [-]

-150.0 °C

0.28 [-]

Show Material materials with Poisson's ratio of 0.28 [-]

-100.0 °C

0.28 [-]

Show Material materials with Poisson's ratio of 0.28 [-]

-50.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

27.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Unlock all property charts

Shear modulus

-269.0 °C

81.7 GPa

Show Material materials with Shear modulus of 81.7 GPa

-200.0 °C

81.8 GPa

Show Material materials with Shear modulus of 81.8 GPa

-150.0 °C

81.1 GPa

Show Material materials with Shear modulus of 81.1 GPa

-100.0 °C

80.2 GPa

Show Material materials with Shear modulus of 80.2 GPa

-50.0 °C

79 GPa

Show Material materials with Shear modulus of 79 GPa

27.0 °C

77 GPa

Show Material materials with Shear modulus of 77 GPa

Unlock all property charts

Tensile strength

20.0 °C

510 - 710 MPa

Show Material materials with Tensile strength of 510 - 710 MPa

Tensile strength, transverse

20.0 °C

510 - 710 MPa

Show Material materials with Tensile strength, transverse of 510 - 710 MPa

Yield strength Rp0.2

20.0 °C

390 MPa

Show Material materials with Yield strength Rp0.2 of 390 MPa

100.0 °C

260 MPa

Show Material materials with Yield strength Rp0.2 of 260 MPa

200.0 °C

220 MPa

Show Material materials with Yield strength Rp0.2 of 220 MPa

250.0 °C

200 MPa

Show Material materials with Yield strength Rp0.2 of 200 MPa

300.0 °C

180 MPa

Show Material materials with Yield strength Rp0.2 of 180 MPa

Unlock all property charts

Yield strength Rp0.2, transverse

20.0 °C

390 MPa

Show Material materials with Yield strength Rp0.2, transverse of 390 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

-100.0 °C

1.02E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.02E-5 1/K

20.0 °C

1.12E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.12E-5 1/K

100.0 °C

1.17E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.17E-5 1/K

200.0 °C

1.21E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.21E-5 1/K

300.0 °C

1.25E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.25E-5 1/K

400.0 °C

1.28E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.28E-5 1/K

Unlock all property charts

Melting point

1316 - 1595 °C

Show Material materials with Melting point of 1316 - 1595 °C

Typical for Nickel Steel

Specific heat capacity

-100.0 °C

440 J/(kg·K)

Show Material materials with Specific heat capacity of 440 J/(kg·K)

20.0 °C

463 J/(kg·K)

Show Material materials with Specific heat capacity of 463 J/(kg·K)

100.0 °C

477 J/(kg·K)

Show Material materials with Specific heat capacity of 477 J/(kg·K)

200.0 °C

494 J/(kg·K)

Show Material materials with Specific heat capacity of 494 J/(kg·K)

300.0 °C

510 J/(kg·K)

Show Material materials with Specific heat capacity of 510 J/(kg·K)

400.0 °C

529 J/(kg·K)

Show Material materials with Specific heat capacity of 529 J/(kg·K)

Unlock all property charts

Thermal conductivity

-100.0 °C

29.5 W/(m·K)

Show Material materials with Thermal conductivity of 29.5 W/(m·K)

20.0 °C

36.2 W/(m·K)

Show Material materials with Thermal conductivity of 36.2 W/(m·K)

100.0 °C

38.5 W/(m·K)

Show Material materials with Thermal conductivity of 38.5 W/(m·K)

200.0 °C

39 W/(m·K)

Show Material materials with Thermal conductivity of 39 W/(m·K)

300.0 °C

38.3 W/(m·K)

Show Material materials with Thermal conductivity of 38.3 W/(m·K)

400.0 °C

36.2 W/(m·K)

Show Material materials with Thermal conductivity of 36.2 W/(m·K)

Unlock all property charts

Thermal diffusivity

20.0 °C

10 mm²/s

Show Material materials with Thermal diffusivity of 10 mm²/s

100.0 °C

10 mm²/s

Show Material materials with Thermal diffusivity of 10 mm²/s

200.0 °C

9.6 mm²/s

Show Material materials with Thermal diffusivity of 9.6 mm²/s

300.0 °C

8.8 mm²/s

Show Material materials with Thermal diffusivity of 8.8 mm²/s

400.0 °C

7.7 mm²/s

Show Material materials with Thermal diffusivity of 7.7 mm²/s

Unlock all property charts

Electrical

PropertyTemperatureValue

Electrical resistivity

-100.0 °C

1.95E-7 Ω·m

Show Material materials with Electrical resistivity of 1.95E-7 Ω·m

20.0 °C

2.61E-7 Ω·m

Show Material materials with Electrical resistivity of 2.61E-7 Ω·m

100.0 °C

3.1E-7 Ω·m

Show Material materials with Electrical resistivity of 3.1E-7 Ω·m

200.0 °C

3.78E-7 Ω·m

Show Material materials with Electrical resistivity of 3.78E-7 Ω·m

300.0 °C

4.57E-7 Ω·m

Show Material materials with Electrical resistivity of 4.57E-7 Ω·m

400.0 °C

5.57E-7 Ω·m

Show Material materials with Electrical resistivity of 5.57E-7 Ω·m

Unlock all property charts

Chemical properties

PropertyValue

Carbon

0.15 %

Show Material materials with Carbon of 0.15 %

Copper

0.3 %

Show Material materials with Copper of 0.3 %

Manganese

0.3 - 0.8 %

Show Material materials with Manganese of 0.3 - 0.8 %

Nickel

4.5 - 5.3 %

Show Material materials with Nickel of 4.5 - 5.3 %

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

Silicon

0.35 %

Show Material materials with Silicon of 0.35 %

Sulfur

0.005 - 0.01 %

Show Material materials with Sulfur of 0.005 - 0.01 %

Vanadium

0.05 %

Show Material materials with Vanadium of 0.05 %