EN 10273 Grade P355QH quenched and tempered (+QT)

Want to keep this datasheet? Save it now in your required format

Description

The steel P355QH is a high temperature steel suitable for welding. Application: use in pressure vessel engineering.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.85 g/cm³

Show Material materials with Density of 7.85 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

190 - 210 GPa

Show Material materials with Elastic modulus of 190 - 210 GPa

Typical for Steel

Elongation

20.0 °C

22 %

Show Material materials with Elongation of 22 %

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Tensile strength

20.0 °C

450 - 630 MPa

Show Material materials with Tensile strength of 450 - 630 MPa

Yield strength

20.0 °C

315 - 355 MPa

Show Material materials with Yield strength of 315 - 355 MPa

Yield strength Rp0.2

50.0 °C

280 - 340 MPa

Show Material materials with Yield strength Rp0.2 of 280 - 340 MPa

100.0 °C

250 - 310 MPa

Show Material materials with Yield strength Rp0.2 of 250 - 310 MPa

150.0 °C

225 - 285 MPa

Show Material materials with Yield strength Rp0.2 of 225 - 285 MPa

200.0 °C

200 - 260 MPa

Show Material materials with Yield strength Rp0.2 of 200 - 260 MPa

250.0 °C

175 - 235 MPa

Show Material materials with Yield strength Rp0.2 of 175 - 235 MPa

300.0 °C

155 - 215 MPa

Show Material materials with Yield strength Rp0.2 of 155 - 215 MPa

Chemical properties

PropertyValue

Aluminium

0.018 %

Show Material materials with Aluminium of 0.018 %

Boron

5E-3 %

Show Material materials with Boron of 5E-3 %

Carbon

0.16 %

Show Material materials with Carbon of 0.16 %

Chromium

0.3 %

Show Material materials with Chromium of 0.3 %

Copper

0.3 %

Show Material materials with Copper of 0.3 %

Manganese

1.5 %

Show Material materials with Manganese of 1.5 %

Molybdenum

0.25 %

Show Material materials with Molybdenum of 0.25 %

Nickel

0.5 %

Show Material materials with Nickel of 0.5 %

Niobium

0.05 %

Show Material materials with Niobium of 0.05 %

Nitrogen

0.02 %

Show Material materials with Nitrogen of 0.02 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.4 %

Show Material materials with Silicon of 0.4 %

Sulfur

0.01 - 0.015 %

Show Material materials with Sulfur of 0.01 - 0.015 %

Titanium

0.03 %

Show Material materials with Titanium of 0.03 %

Vanadium

0.06 %

Show Material materials with Vanadium of 0.06 %

Zirconium

0.05 %

Show Material materials with Zirconium of 0.05 %