EN 10137-2 Grade S460QL quenched and tempered (+QT)

Want to keep this datasheet? Save it now in your required format

Description

S460QL is a tempered and weldable fine grained steel. yield point: >460 N/mm² application: welded steel constructions of various types, e.g. bridges and load-carrying constructions as well as transport vehicles, lifting and earthmoving machines. application limits: at -40°C is warranted a notch impact energy of 30 J (longitudinal test specimen) cold formability: for nominal size < 16 mm bending radius in transversal direction 3xs in longitudinal direction 4xs (s= nominal thickness) hot forming property: allowed only for stress relieve annealing temperature (max. 580°C) suitability for welding: Steel is weldable according to the common welding methods (EURONORM-INFORMATION Nr. 2 has to be considered)

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Typical for Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

190 - 210 GPa

Show Material materials with Elastic modulus of 190 - 210 GPa

Typical for Steel

Elongation

20.0 °C

17 %

Show Material materials with Elongation of 17 %

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Tensile strength

20.0 °C

500 - 720 MPa

Show Material materials with Tensile strength of 500 - 720 MPa

Yield strength

20.0 °C

400 - 460 MPa

Show Material materials with Yield strength of 400 - 460 MPa

Chemical properties

PropertyValue

Boron

5E-3 %

Show Material materials with Boron of 5E-3 %

Carbon

0.2 %

Show Material materials with Carbon of 0.2 %

Chromium

1.5 %

Show Material materials with Chromium of 1.5 %

Copper

0.5 %

Show Material materials with Copper of 0.5 %

Manganese

1.7 %

Show Material materials with Manganese of 1.7 %

Molybdenum

0.7 %

Show Material materials with Molybdenum of 0.7 %

Nickel

2 %

Show Material materials with Nickel of 2 %

Niobium

0.06 %

Show Material materials with Niobium of 0.06 %

Nitrogen

0.02 %

Show Material materials with Nitrogen of 0.02 %

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

Silicon

0.8 %

Show Material materials with Silicon of 0.8 %

Sulfur

0.01 - 0.015 %

Show Material materials with Sulfur of 0.01 - 0.015 %

Titanium

0.05 %

Show Material materials with Titanium of 0.05 %

Vanadium

0.12 %

Show Material materials with Vanadium of 0.12 %

Zirconium

0.15 %

Show Material materials with Zirconium of 0.15 %