EN 10025-6 Grade S960QL quenched and tempered (+QT)

View suppliers (7)
Want to keep this datasheet? Save it now in your required format

Description

S960QL is a tempered and weldable fine grained steel. yield point: >960 N/mm² application: welded steel constructions of various types, e.g. bridges and load-carrying constructions as well as transport vehicles, lifting and earthmoving machines. application limits: at -40°C is warranted a notch impact energy of 30 J (longitudinal test specimen) cold formability: for nominal size < 16 mm bending radius in transversal direction 3xs in longitudinal direction 4xs (s= nominal thickness) hot forming property: allowed only for stress relieve annealing temperature (max. 580°C) suitability for welding: Steel is weldable according to the common welding methods (EURONORM-INFORMATION Nr. 2 has to be considered)

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

20 °C

7.84 g/cm³

Show Material materials with Density of 7.84 g/cm³

quenched and tempered (+QT)

EN 10025-6, EN 10113-3

Flat

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

20 °C

210 GPa

Show Material materials with Elastic modulus of 210 GPa

quenched and tempered (+QT)

EN 10025-6, EN 10113-3

Flat

Elongation

10.5 %

Show Material materials with Elongation of 10.5 %

Predicted Value, A80

10.8 %

Show Material materials with Elongation of 10.8 %

Predicted Value, A50

12.6 %

Show Material materials with Elongation of 12.6 %

Predicted Value, A200

12.6 %

Show Material materials with Elongation of 12.6 %

Predicted Value, Transverse

17.8 %

Show Material materials with Elongation of 17.8 %

Predicted Value, A5

18.3 %

Show Material materials with Elongation of 18.3 %

Predicted Value, A80 Transverse

20 °C

10 %

Show Material materials with Elongation of 10 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6, EN 10113-3

Sheet, Flat

Poisson's ratio

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Tensile strength

20 °C

980 - 1150 MPa

Show Material materials with Tensile strength of 980 - 1150 MPa

quenched and tempered (+QT)

EN 10137-2, EN 10025-6, EN 10113-3

Sheet, Flat

Yield strength

313.5 MPa

Show Material materials with Yield strength of 313.5 MPa

Predicted Value, RP1

329.7 MPa

Show Material materials with Yield strength of 329.7 MPa

Predicted Value, RP1 Transverse

541.7 MPa

Show Material materials with Yield strength of 541.7 MPa

Predicted Value, RP05

604.8 MPa

Show Material materials with Yield strength of 604.8 MPa

Predicted Value, RP02 Transverse

616.3 MPa

Show Material materials with Yield strength of 616.3 MPa

Predicted Value, Transverse

800.6 MPa

Show Material materials with Yield strength of 800.6 MPa

Predicted Value, RP002

858.3 MPa

Show Material materials with Yield strength of 858.3 MPa

Predicted Value, RP02

20 °C

960 MPa

Show Material materials with Yield strength of 960 MPa

quenched and tempered (+QT)

EN 10137-2, EN 10025-6, EN 10113-3

Sheet, Flat

Thermal

PropertyTemperatureValueConditionRelated StandardsShape

Coefficient of thermal expansion

100 °C

1.2e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.2e-05 1/K

quenched and tempered (+QT)

EN 10025-6, EN 10113-3

Flat

Specific heat capacity

20 °C

440 J/(kg·K)

Show Material materials with Specific heat capacity of 440 J/(kg·K)

quenched and tempered (+QT)

EN 10025-6, EN 10113-3

Flat

Thermal conductivity

20 °C

38 W/(m·K)

Show Material materials with Thermal conductivity of 38 W/(m·K)

quenched and tempered (+QT)

EN 10025-6, EN 10113-3

Flat

Electrical

PropertyTemperatureValueConditionRelated StandardsShape

Electrical resistivity

20 °C

2.8e-07 Ω·m

Show Material materials with Electrical resistivity of 2.8e-07 Ω·m

quenched and tempered (+QT)

EN 10025-6, EN 10113-3

Flat

Chemical properties

PropertyValueConditionRelated StandardsShape

Boron

0.005 %

Show Material materials with Boron of 0.005 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6, EN 10113-3

Sheet, Flat

Carbon

0.2 %

Show Material materials with Carbon of 0.2 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6, EN 10113-3

Sheet, Flat

Chromium

1.5 %

Show Material materials with Chromium of 1.5 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6, EN 10113-3

Sheet, Flat

Copper

0.5 %

Show Material materials with Copper of 0.5 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6, EN 10113-3

Sheet, Flat

Manganese

1.7 %

Show Material materials with Manganese of 1.7 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6, EN 10113-3

Sheet, Flat

Molybdenum

0.7 %

Show Material materials with Molybdenum of 0.7 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6, EN 10113-3

Sheet, Flat

Nickel

2 %

Show Material materials with Nickel of 2 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6, EN 10113-3

Sheet, Flat

Niobium

0.06 %

Show Material materials with Niobium of 0.06 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6, EN 10113-3

Sheet, Flat

Nitrogen

0.015 %

Show Material materials with Nitrogen of 0.015 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6, EN 10113-3

Sheet, Flat

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6, EN 10113-3

Sheet, Flat

Silicon

0.8 %

Show Material materials with Silicon of 0.8 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6, EN 10113-3

Sheet, Flat

Sulfur

0.01 %

Show Material materials with Sulfur of 0.01 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6, EN 10113-3

Sheet, Flat

Titanium

0.05 %

Show Material materials with Titanium of 0.05 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6, EN 10113-3

Sheet, Flat

Vanadium

0.12 %

Show Material materials with Vanadium of 0.12 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6, EN 10113-3

Sheet, Flat

Zirconium

0.15 %

Show Material materials with Zirconium of 0.15 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6, EN 10113-3

Sheet, Flat

Technological properties

Property
Supplier Disclaimer

The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information.