Description

High-temperature steel for screws and nuts. Max. application temperature: 540 °C Further application for mounting elements at increased temperatures.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.83 - 7.85 g/cm³

Show Material materials with Density of 7.83 - 7.85 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

-100.0 °C

217 GPa

Show Material materials with Elastic modulus of 217 GPa

20.0 °C

211 - 212 GPa

Show Material materials with Elastic modulus of 211 - 212 GPa

100.0 °C

204 - 207 GPa

Show Material materials with Elastic modulus of 204 - 207 GPa

200.0 °C

196 - 199 GPa

Show Material materials with Elastic modulus of 196 - 199 GPa

300.0 °C

186 - 192 GPa

Show Material materials with Elastic modulus of 186 - 192 GPa

400.0 °C

177 - 184 GPa

Show Material materials with Elastic modulus of 177 - 184 GPa

500.0 °C

164 - 175 GPa

Show Material materials with Elastic modulus of 164 - 175 GPa

600.0 °C

127 - 164 GPa

Show Material materials with Elastic modulus of 127 - 164 GPa

Elongation

20.0 °C

14 %

Show Material materials with Elongation of 14 %

Poisson's ratio

20.0 °C

0.28 [-]

Show Material materials with Poisson's ratio of 0.28 [-]

Reduction of area

20.0 °C

45 %

Show Material materials with Reduction of area of 45 %

Tensile strength

20.0 °C

850 - 1000 MPa

Show Material materials with Tensile strength of 850 - 1000 MPa

Yield strength Rp0.2

20.0 °C

640 - 700 MPa

Show Material materials with Yield strength Rp0.2 of 640 - 700 MPa

50.0 °C

631 - 687 MPa

Show Material materials with Yield strength Rp0.2 of 631 - 687 MPa

100.0 °C

612 - 670 MPa

Show Material materials with Yield strength Rp0.2 of 612 - 670 MPa

150.0 °C

591 - 647 MPa

Show Material materials with Yield strength Rp0.2 of 591 - 647 MPa

200.0 °C

577 - 631 MPa

Show Material materials with Yield strength Rp0.2 of 577 - 631 MPa

250.0 °C

556 - 608 MPa

Show Material materials with Yield strength Rp0.2 of 556 - 608 MPa

300.0 °C

542 - 593 MPa

Show Material materials with Yield strength Rp0.2 of 542 - 593 MPa

350.0 °C

528 - 577 MPa

Show Material materials with Yield strength Rp0.2 of 528 - 577 MPa

400.0 °C

507 - 554 MPa

Show Material materials with Yield strength Rp0.2 of 507 - 554 MPa

450.0 °C

479 - 523 MPa

Show Material materials with Yield strength Rp0.2 of 479 - 523 MPa

500.0 °C

429 - 470 MPa

Show Material materials with Yield strength Rp0.2 of 429 - 470 MPa

550.0 °C

366 - 400 MPa

Show Material materials with Yield strength Rp0.2 of 366 - 400 MPa

600.0 °C

268 - 293 MPa

Show Material materials with Yield strength Rp0.2 of 268 - 293 MPa

Unlock all property charts

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

-100.0 °C

1.05E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.05E-5 1/K

20.0 °C

1.15E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.15E-5 1/K

100.0 °C

1.11E-5 - 1.21E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.11E-5 - 1.21E-5 1/K

200.0 °C

1.21E-5 - 1.27E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.21E-5 - 1.27E-5 1/K

300.0 °C

1.29E-5 - 1.32E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.29E-5 - 1.32E-5 1/K

400.0 °C

1.35E-5 - 1.36E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.35E-5 - 1.36E-5 1/K

500.0 °C

1.39E-5 - 1.4E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.39E-5 - 1.4E-5 1/K

600.0 °C

1.41E-5 - 1.44E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.41E-5 - 1.44E-5 1/K

Unlock all property charts

Max service temperature, long

0 - 540 °C

Show Material materials with Max service temperature, long of 0 - 540 °C

Melting point

1382 - 1529 °C

Show Material materials with Melting point of 1382 - 1529 °C

Typical for Chromium Molybdenum Steel

Specific heat capacity

-100.0 °C

423 J/(kg·K)

Show Material materials with Specific heat capacity of 423 J/(kg·K)

20.0 °C

460 - 461 J/(kg·K)

Show Material materials with Specific heat capacity of 460 - 461 J/(kg·K)

100.0 °C

479 J/(kg·K)

Show Material materials with Specific heat capacity of 479 J/(kg·K)

200.0 °C

499 J/(kg·K)

Show Material materials with Specific heat capacity of 499 J/(kg·K)

300.0 °C

517 J/(kg·K)

Show Material materials with Specific heat capacity of 517 J/(kg·K)

400.0 °C

536 J/(kg·K)

Show Material materials with Specific heat capacity of 536 J/(kg·K)

500.0 °C

558 J/(kg·K)

Show Material materials with Specific heat capacity of 558 J/(kg·K)

600.0 °C

587 J/(kg·K)

Show Material materials with Specific heat capacity of 587 J/(kg·K)

Unlock all property charts

Thermal conductivity

20.0 °C

33 - 45.1 W/(m·K)

Show Material materials with Thermal conductivity of 33 - 45.1 W/(m·K)

100.0 °C

45.1 W/(m·K)

Show Material materials with Thermal conductivity of 45.1 W/(m·K)

200.0 °C

44.1 W/(m·K)

Show Material materials with Thermal conductivity of 44.1 W/(m·K)

300.0 °C

41.9 W/(m·K)

Show Material materials with Thermal conductivity of 41.9 W/(m·K)

400.0 °C

39.4 W/(m·K)

Show Material materials with Thermal conductivity of 39.4 W/(m·K)

500.0 °C

36.9 W/(m·K)

Show Material materials with Thermal conductivity of 36.9 W/(m·K)

600.0 °C

34.4 W/(m·K)

Show Material materials with Thermal conductivity of 34.4 W/(m·K)

Unlock all property charts

Thermal diffusivity

20.0 °C

12.5 mm²/s

Show Material materials with Thermal diffusivity of 12.5 mm²/s

100.0 °C

11.6 mm²/s

Show Material materials with Thermal diffusivity of 11.6 mm²/s

200.0 °C

10.6 mm²/s

Show Material materials with Thermal diffusivity of 10.6 mm²/s

300.0 °C

9.5 mm²/s

Show Material materials with Thermal diffusivity of 9.5 mm²/s

400.0 °C

8.4 mm²/s

Show Material materials with Thermal diffusivity of 8.4 mm²/s

500.0 °C

7.1 mm²/s

Show Material materials with Thermal diffusivity of 7.1 mm²/s

600.0 °C

5.8 mm²/s

Show Material materials with Thermal diffusivity of 5.8 mm²/s

Unlock all property charts

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

2.31E-7 Ω·m

Show Material materials with Electrical resistivity of 2.31E-7 Ω·m

100.0 °C

2.84E-7 Ω·m

Show Material materials with Electrical resistivity of 2.84E-7 Ω·m

200.0 °C

3.58E-7 Ω·m

Show Material materials with Electrical resistivity of 3.58E-7 Ω·m

300.0 °C

4.48E-7 Ω·m

Show Material materials with Electrical resistivity of 4.48E-7 Ω·m

400.0 °C

5.52E-7 Ω·m

Show Material materials with Electrical resistivity of 5.52E-7 Ω·m

500.0 °C

6.71E-7 Ω·m

Show Material materials with Electrical resistivity of 6.71E-7 Ω·m

600.0 °C

8.06E-7 Ω·m

Show Material materials with Electrical resistivity of 8.06E-7 Ω·m

Unlock all property charts

Chemical properties

PropertyValue

Aluminium

0.015 %

Show Material materials with Aluminium of 0.015 %

Carbon

0.36 - 0.44 %

Show Material materials with Carbon of 0.36 - 0.44 %

Chromium

0.9 - 1.2 %

Show Material materials with Chromium of 0.9 - 1.2 %

Manganese

0.45 - 0.85 %

Show Material materials with Manganese of 0.45 - 0.85 %

Molybdenum

0.5 - 0.65 %

Show Material materials with Molybdenum of 0.5 - 0.65 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.4 %

Show Material materials with Silicon of 0.4 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %

Vanadium

0.25 - 0.35 %

Show Material materials with Vanadium of 0.25 - 0.35 %