General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Low Carbon Steel |
Hardness, Vickers | 23.0 °C | 117 - 172 [-] Show Material materials with Hardness, Vickers of 117 - 172 [-] | |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Low Carbon Steel |
Shear modulus | 23.0 °C | 82 GPa Show Material materials with Shear modulus of 82 GPa | Typical for Low Carbon Steel |
Tensile strength | 23.0 °C | 390 - 540 MPa Show Material materials with Tensile strength of 390 - 540 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.32E-5 - 1.38E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.32E-5 - 1.38E-5 1/K | Typical for Low Carbon Steel |
Max service temperature | 500 °C Show Material materials with Max service temperature of 500 °C | Typical for Carbon Steel | |
Melting point | 1480 - 1526 °C Show Material materials with Melting point of 1480 - 1526 °C | Typical for Low Carbon Steel | |
Specific heat capacity | 23.0 °C | 465 J/(kg·K) Show Material materials with Specific heat capacity of 465 J/(kg·K) | Typical for Low Carbon Steel |
Thermal conductivity | 23.0 °C | 22 W/(m·K) Show Material materials with Thermal conductivity of 22 W/(m·K) |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 23.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Magnetic
Property | Value | Comment |
---|---|---|
Curie temperature | 770 °C Show Material materials with Curie temperature of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | General Automotive Parts , Tubes, Furniture, Radiators, Electrical goods, Domestic Appliances, Construction |
Do you have a technical question or need more information about this material?