Properties

Mechanical

PropertyTemperatureValue

Elongation A5

20.0 °C

35 %

Show Material materials with Elongation A5 of 35 %

Tensile strength

20.0 °C

520 - 550 MPa

Show Material materials with Tensile strength of 520 - 550 MPa

Yield strength Rp0.2

20.0 °C

175 - 205 MPa

Show Material materials with Yield strength Rp0.2 of 175 - 205 MPa

Chemical properties

PropertyValue

Carbon

0.15 %

Show Material materials with Carbon of 0.15 %

Chromium

14 - 17 %

Show Material materials with Chromium of 14 - 17 %

Copper

0.5 %

Show Material materials with Copper of 0.5 %

Iron

6 - 10 %

Show Material materials with Iron of 6 - 10 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Nickel

72 %

Show Material materials with Nickel of 72 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.5 %

Show Material materials with Silicon of 0.5 %

Sulfur

0.015 %

Show Material materials with Sulfur of 0.015 %

Technological properties

Property
Processing history