Properties

Mechanical

PropertyTemperatureValue

Elongation A5

20.0 °C

30 %

Show Material materials with Elongation A5 of 30 %

Tensile strength

20.0 °C

450 MPa

Show Material materials with Tensile strength of 450 MPa

Yield strength Rp0.2

20.0 °C

175 MPa

Show Material materials with Yield strength Rp0.2 of 175 MPa

Chemical properties

PropertyValue

Aluminium

0.15 - 0.6 %

Show Material materials with Aluminium of 0.15 - 0.6 %

Carbon

0.1 %

Show Material materials with Carbon of 0.1 %

Chromium

19 - 23 %

Show Material materials with Chromium of 19 - 23 %

Copper

0.75 %

Show Material materials with Copper of 0.75 %

Iron

37.4 - 50.7 %

Show Material materials with Iron of 37.4 - 50.7 %

Manganese

1.5 %

Show Material materials with Manganese of 1.5 %

Nickel

30 - 35 %

Show Material materials with Nickel of 30 - 35 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Sulfur

0.015 %

Show Material materials with Sulfur of 0.015 %

Titanium

0.15 - 0.6 %

Show Material materials with Titanium of 0.15 - 0.6 %

Technological properties

Property
Processing history

hot-finished, annealed