JIS G4903 Grade NCF825TP hot-finished, annealed

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by Japanese Industrial Standards.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation A5

20.0 °C

30 %

Show Material materials with Elongation A5 of 30 %

Tensile strength

20.0 °C

520 MPa

Show Material materials with Tensile strength of 520 MPa

Yield strength Rp0.2

20.0 °C

175 MPa

Show Material materials with Yield strength Rp0.2 of 175 MPa

Chemical properties

PropertyValue

Aluminium

0.2 %

Show Material materials with Aluminium of 0.2 %

Carbon

0.05 %

Show Material materials with Carbon of 0.05 %

Chromium

19.5 - 23.5 %

Show Material materials with Chromium of 19.5 - 23.5 %

Copper

1.5 - 3 %

Show Material materials with Copper of 1.5 - 3 %

Iron

21 - 37.9 %

Show Material materials with Iron of 21 - 37.9 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Molybdenum

2.5 - 3.5 %

Show Material materials with Molybdenum of 2.5 - 3.5 %

Nickel

38 - 46 %

Show Material materials with Nickel of 38 - 46 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.5 %

Show Material materials with Silicon of 0.5 %

Sulfur

0.015 %

Show Material materials with Sulfur of 0.015 %

Titanium

0.6 - 1.2 %

Show Material materials with Titanium of 0.6 - 1.2 %

Technological properties

Property
Processing history

hot-finished, annealed