General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation A5 | 23.0 °C | 40 % Show Material materials with Elongation A5 of 40 % | |
Hardness, Brinell | 23.0 °C | 201 [-] Show Material materials with Hardness, Brinell of 201 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Reduction of area | 23.0 °C | 50 % Show Material materials with Reduction of area of 50 % | |
Tensile strength | 23.0 °C | 560 MPa Show Material materials with Tensile strength of 560 MPa | |
Yield strength Rp0.2 | 23.0 °C | 205 MPa Show Material materials with Yield strength Rp0.2 of 205 MPa |
Technological properties
Property | ||
---|---|---|
Processing history | solution treated |