JIS G4315 Grade SUS660-WSB

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by Japanese Industrial Standards.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation A5

20.0 °C

8 - 10 %

Show Material materials with Elongation A5 of 8 - 10 %

Reduction of area

20.0 °C

60 %

Show Material materials with Reduction of area of 60 %

Tensile strength

20.0 °C

600 - 830 MPa

Show Material materials with Tensile strength of 600 - 830 MPa

Chemical properties

PropertyValue

Aluminium

0.35 %

Show Material materials with Aluminium of 0.35 %

Boron

0.001 - 0.01 %

Show Material materials with Boron of 0.001 - 0.01 %

Carbon

0.08 %

Show Material materials with Carbon of 0.08 %

Chromium

13.5 - 16 %

Show Material materials with Chromium of 13.5 - 16 %

Iron

49.13 - 59.5 %

Show Material materials with Iron of 49.13 - 59.5 %

Manganese

2 %

Show Material materials with Manganese of 2 %

Molybdenum

1 - 1.5 %

Show Material materials with Molybdenum of 1 - 1.5 %

Nickel

24 - 27 %

Show Material materials with Nickel of 24 - 27 %

Phosphorus

0.05 %

Show Material materials with Phosphorus of 0.05 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %

Titanium

1.9 %

Show Material materials with Titanium of 1.9 %

Vanadium

0.1 - 0.5 %

Show Material materials with Vanadium of 0.1 - 0.5 %