JIS G4315 Grade SUSXM7-WSB

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by Japanese Industrial Standards.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation A5

20.0 °C

20 - 25 %

Show Material materials with Elongation A5 of 20 - 25 %

Reduction of area

20.0 °C

65 %

Show Material materials with Reduction of area of 65 %

Tensile strength

20.0 °C

450 - 680 MPa

Show Material materials with Tensile strength of 450 - 680 MPa

Chemical properties

PropertyValue

Carbon

0.08 %

Show Material materials with Carbon of 0.08 %

Chromium

17 - 19 %

Show Material materials with Chromium of 17 - 19 %

Copper

3 - 4 %

Show Material materials with Copper of 3 - 4 %

Iron

63.34 - 71.5 %

Show Material materials with Iron of 63.34 - 71.5 %

Manganese

2 %

Show Material materials with Manganese of 2 %

Nickel

8.5 - 10.5 %

Show Material materials with Nickel of 8.5 - 10.5 %

Phosphorus

0.05 %

Show Material materials with Phosphorus of 0.05 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %