Properties

Mechanical

PropertyTemperatureValue

Elongation A5

23.0 °C

30 %

Show Material materials with Elongation A5 of 30 %

Hardness, Brinell

23.0 °C

207 [-]

Show Material materials with Hardness, Brinell of 207 [-]

Hardness, Rockwell B

23.0 °C

96 [-]

Show Material materials with Hardness, Rockwell B of 96 [-]

Hardness, Vickers

23.0 °C

214 [-]

Show Material materials with Hardness, Vickers of 214 [-]

Tensile strength

23.0 °C

580 MPa

Show Material materials with Tensile strength of 580 MPa

Yield strength Rp0.2

23.0 °C

235 MPa

Show Material materials with Yield strength Rp0.2 of 235 MPa

Technological properties

Property
Processing history

solution treated