General
Property | Value | Temperature | Comment |
---|---|---|---|
Density | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ at 23.0 °C | 23.0 °C | Typical for Low Carbon Steel |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elastic modulus | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa at 23.0 °C | 23.0 °C | Typical for Low Carbon Steel |
Elongation | 25 % Show Material materials with Elongation of 25 % at 23.0 °C | 23.0 °C | |
Elongation A50 | 25 % Show Material materials with Elongation A50 of 25 % at 23.0 °C | 23.0 °C | |
Poisson's ratio | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] at 23.0 °C | 23.0 °C | Typical for Low Carbon Steel |
Shear modulus | 82 GPa Show Material materials with Shear modulus of 82 GPa at 23.0 °C | 23.0 °C | Typical for Low Carbon Steel |
Tensile strength | 450 MPa Show Material materials with Tensile strength of 450 MPa at 23.0 °C | 23.0 °C | |
Yield strength | 310 MPa Show Material materials with Yield strength of 310 MPa at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature | Comment |
---|---|---|---|
Coefficient of thermal expansion | 1.32E-5 - 1.38E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.32E-5 - 1.38E-5 1/K at 23.0 °C | 23.0 °C | Typical for Low Carbon Steel |
Max service temperature | 500 °C Show Material materials with Max service temperature of 500 °C | Typical for Carbon Steel | |
Melting point | 1480 - 1526 °C Show Material materials with Melting point of 1480 - 1526 °C | Typical for Low Carbon Steel | |
Specific heat capacity | 465 J/(kg·K) Show Material materials with Specific heat capacity of 465 J/(kg·K) at 23.0 °C | 23.0 °C | Typical for Low Carbon Steel |
Thermal conductivity | 25 - 93 W/(m·K) Show Material materials with Thermal conductivity of 25 - 93 W/(m·K) at 23.0 °C | 23.0 °C | Typical for Low Carbon Steel |
Electrical
Property | Value | Temperature | Comment |
---|---|---|---|
Electrical resistivity | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m at 23.0 °C | 23.0 °C | Typical for Carbon Steel |
Magnetic
Property | Value | Comment |
---|---|---|
Curie temperature | 770 °C Show Material materials with Curie temperature of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | ||
---|---|---|
Carbon | 0.22 % | |
Iron | 98.53 - 100 % | balance |
Manganese | 1.25 % |
Technological properties
Property | ||
---|---|---|
Processing history | hot-rolled |