Mechanical

PropertyTemperatureValue

Hardness, Brinell

20.0 °C

217 [-]

Show Material materials with Hardness, Brinell of 217 [-]

Hardness, Rockwell B

20.0 °C

97 [-]

Show Material materials with Hardness, Rockwell B of 97 [-]

Chemical properties

PropertyValue

Aluminium

0.05 %

Show Material materials with Aluminium of 0.05 %

Carbon

0.85 - 1 %

Show Material materials with Carbon of 0.85 - 1 %

Chromium

1.4 - 1.8 %

Show Material materials with Chromium of 1.4 - 1.8 %

Copper

0.3 %

Show Material materials with Copper of 0.3 %

Manganese

1.4 - 1.7 %

Show Material materials with Manganese of 1.4 - 1.7 %

Molybdenum

0.1 %

Show Material materials with Molybdenum of 0.1 %

Nickel

0.25 %

Show Material materials with Nickel of 0.25 %

Oxygen

1.5E-3 %

Show Material materials with Oxygen of 1.5E-3 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.5 - 0.8 %

Show Material materials with Silicon of 0.5 - 0.8 %

Sulfur

0.015 %

Show Material materials with Sulfur of 0.015 %

Titanium

5E-3 %

Show Material materials with Titanium of 5E-3 %