Mechanical
Property | Temperature | Value |
---|---|---|
Hardness, Brinell | 20.0 °C | 260 [-] Show Material materials with Hardness, Brinell of 260 [-] |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Carbon | 0.85 - 1 % Show Material materials with Carbon of 0.85 - 1 % |
Chromium | 1.4 - 1.8 % Show Material materials with Chromium of 1.4 - 1.8 % |
Copper | 0.3 % Show Material materials with Copper of 0.3 % |
Manganese | 1.4 - 1.7 % Show Material materials with Manganese of 1.4 - 1.7 % |
Molybdenum | 0.1 % Show Material materials with Molybdenum of 0.1 % |
Nickel | 0.25 % Show Material materials with Nickel of 0.25 % |
Oxygen | 1.5E-3 % Show Material materials with Oxygen of 1.5E-3 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.5 - 0.8 % Show Material materials with Silicon of 0.5 - 0.8 % |
Sulfur | 0.015 % Show Material materials with Sulfur of 0.015 % |
Titanium | 5E-3 % Show Material materials with Titanium of 5E-3 % |