General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Chromium Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Chromium Steel |
Hardness, Brinell | 20.0 °C | 260 [-] Show Material materials with Hardness, Brinell of 260 [-] | |
Poisson's ratio | 20.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Chromium Steel |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 20.0 °C | 9.4E-6 - 1.5E-5 1/K Show Material materials with Coefficient of thermal expansion of 9.4E-6 - 1.5E-5 1/K | Typical for Chromium Steel |
Melting point | 1382 - 1529 °C Show Material materials with Melting point of 1382 - 1529 °C | Typical for Chromium Steel | |
Specific heat capacity | 20.0 °C | 440 - 494 J/(kg·K) Show Material materials with Specific heat capacity of 440 - 494 J/(kg·K) | Typical for Chromium Steel |
Thermal conductivity | 20.0 °C | 23 - 50 W/(m·K) Show Material materials with Thermal conductivity of 23 - 50 W/(m·K) | Typical for Chromium Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Carbon | 0.93 - 1.05 % Show Material materials with Carbon of 0.93 - 1.05 % |
Chromium | 1.65 - 1.95 % Show Material materials with Chromium of 1.65 - 1.95 % |
Copper | 0.3 % Show Material materials with Copper of 0.3 % |
Manganese | 0.6 - 0.8 % Show Material materials with Manganese of 0.6 - 0.8 % |
Molybdenum | 0.2 - 0.35 % Show Material materials with Molybdenum of 0.2 - 0.35 % |
Oxygen | 1.5E-3 % Show Material materials with Oxygen of 1.5E-3 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.15 - 0.45 % Show Material materials with Silicon of 0.15 - 0.45 % |
Sulfur | 0.015 % Show Material materials with Sulfur of 0.015 % |