ASTM A31 Grade B Hot- or Cold-Headed or As-Rolled

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation A200

23.0 °C

22 %

Show Material materials with Elongation A200 of 22 %

Elongation A50

23.0 °C

25 %

Show Material materials with Elongation A50 of 25 %

Tensile strength

23.0 °C

400 - 470 MPa

Show Material materials with Tensile strength of 400 - 470 MPa

Yield strength

23.0 °C

200 MPa

Show Material materials with Yield strength of 200 MPa

Chemical properties

PropertyValue

Carbon

0.28 %

Show Material materials with Carbon of 0.28 %

Manganese

0.3 - 0.8 %

Show Material materials with Manganese of 0.3 - 0.8 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Sulfur

0.05 %

Show Material materials with Sulfur of 0.05 %