Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 23.0 °C | 30 % Show Material materials with Elongation A50 of 30 % |
Reduction of area | 23.0 °C | 50 % Show Material materials with Reduction of area of 50 % |
Tensile strength | 23.0 °C | 655 MPa Show Material materials with Tensile strength of 655 MPa |
Yield strength Rp0.2 | 23.0 °C | 310 MPa Show Material materials with Yield strength Rp0.2 of 310 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.03 % Show Material materials with Carbon of 0.03 % |
Chromium | 20 - 22 % Show Material materials with Chromium of 20 - 22 % |
Copper | 0.75 % Show Material materials with Copper of 0.75 % |
Manganese | 2 % Show Material materials with Manganese of 2 % |
Molybdenum | 6 - 7 % Show Material materials with Molybdenum of 6 - 7 % |
Nickel | 23.5 - 25.5 % Show Material materials with Nickel of 23.5 - 25.5 % |
Nitrogen | 0.18 - 0.25 % Show Material materials with Nitrogen of 0.18 - 0.25 % |
Phosphorus | 0.04 % Show Material materials with Phosphorus of 0.04 % |
Silicon | 1 % Show Material materials with Silicon of 1 % |
Sulfur | 0.03 % Show Material materials with Sulfur of 0.03 % |