Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 23.0 °C | 40 % Show Material materials with Elongation A50 of 40 % |
Reduction of area | 23.0 °C | 50 % Show Material materials with Reduction of area of 50 % |
Tensile strength | 23.0 °C | 500 MPa Show Material materials with Tensile strength of 500 MPa |
Yield strength Rp0.2 | 23.0 °C | 214 MPa Show Material materials with Yield strength Rp0.2 of 214 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.03 % Show Material materials with Carbon of 0.03 % |
Chromium | 26 - 28 % Show Material materials with Chromium of 26 - 28 % |
Copper | 0.6 - 1.4 % Show Material materials with Copper of 0.6 - 1.4 % |
Manganese | 2.5 % Show Material materials with Manganese of 2.5 % |
Molybdenum | 3 - 4 % Show Material materials with Molybdenum of 3 - 4 % |
Nickel | 30 - 34 % Show Material materials with Nickel of 30 - 34 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 1 % Show Material materials with Silicon of 1 % |
Sulfur | 0.03 % Show Material materials with Sulfur of 0.03 % |