General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.6 - 7.8 g/cm³ Show Material materials with Density of 7.6 - 7.8 g/cm³ | Typical for Ferritic Stainless Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy | 23.0 °C | 40 J Show Material materials with Charpy impact energy of 40 J | |
Elastic modulus | 23.0 °C | 220 GPa Show Material materials with Elastic modulus of 220 GPa | Typical for Ferritic Stainless Steel |
Elongation A50 | 23.0 °C | 18 % Show Material materials with Elongation A50 of 18 % | |
Hardness, Brinell | 23.0 °C | 269 [-] Show Material materials with Hardness, Brinell of 269 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Ferritic Stainless Steel |
Reduction of area | 23.0 °C | 50 % Show Material materials with Reduction of area of 50 % | |
Shear modulus | 23.0 °C | 77 GPa Show Material materials with Shear modulus of 77 GPa | Typical for Ferritic Stainless Steel |
Tensile strength | 23.0 °C | 760 MPa Show Material materials with Tensile strength of 760 MPa | |
Yield strength Rp0.2 | 23.0 °C | 620 MPa Show Material materials with Yield strength Rp0.2 of 620 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 9.3E-6 - 1.2E-5 1/K Show Material materials with Coefficient of thermal expansion of 9.3E-6 - 1.2E-5 1/K | Typical for Ferritic Stainless Steel |
Melting point | 1425 - 1530 °C Show Material materials with Melting point of 1425 - 1530 °C | Typical for Ferritic Stainless Steel | |
Specific heat capacity | 23.0 °C | 420 - 586 J/(kg·K) Show Material materials with Specific heat capacity of 420 - 586 J/(kg·K) | Typical for Ferritic Stainless Steel |
Thermal conductivity | 23.0 °C | 11 - 22 W/(m·K) Show Material materials with Thermal conductivity of 11 - 22 W/(m·K) | Typical for Ferritic Stainless Steel |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 23.0 °C | 6E-7 - 7.5E-7 Ω·m Show Material materials with Electrical resistivity of 6E-7 - 7.5E-7 Ω·m | Typical for Ferritic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.025 % Show Material materials with Aluminium of 0.025 % |
Carbon | 0.1 - 0.15 % Show Material materials with Carbon of 0.1 - 0.15 % |
Chromium | 11.5 - 13 % Show Material materials with Chromium of 11.5 - 13 % |
Copper | 0.15 % Show Material materials with Copper of 0.15 % |
Manganese | 0.25 - 0.8 % Show Material materials with Manganese of 0.25 - 0.8 % |
Molybdenum | 0.5 % Show Material materials with Molybdenum of 0.5 % |
Nickel | 0.75 % Show Material materials with Nickel of 0.75 % |
Niobium | 0.2 % Show Material materials with Niobium of 0.2 % |
Nitrogen | 0.08 % Show Material materials with Nitrogen of 0.08 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 0.5 % Show Material materials with Silicon of 0.5 % |
Sulfur | 0.015 % Show Material materials with Sulfur of 0.015 % |
Tin | 0.05 % Show Material materials with Tin of 0.05 % |
Titanium | 0.05 % Show Material materials with Titanium of 0.05 % |
Tungsten | 0.1 % Show Material materials with Tungsten of 0.1 % |