General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy | 23.0 °C | 27 J Show Material materials with Charpy impact energy of 27 J | |
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation A50 | 23.0 °C | 15 % Show Material materials with Elongation A50 of 15 % | |
Hardness, Brinell | 23.0 °C | 277 [-] Show Material materials with Hardness, Brinell of 277 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Reduction of area | 23.0 °C | 50 % Show Material materials with Reduction of area of 50 % | |
Tensile strength | 23.0 °C | 795 MPa Show Material materials with Tensile strength of 795 MPa | |
Yield strength Rp0.2 | 23.0 °C | 515 MPa Show Material materials with Yield strength Rp0.2 of 515 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Carbon | 0.13 - 0.18 % Show Material materials with Carbon of 0.13 - 0.18 % |
Chromium | 11.5 - 13 % Show Material materials with Chromium of 11.5 - 13 % |
Manganese | 0.4 - 0.6 % Show Material materials with Manganese of 0.4 - 0.6 % |
Molybdenum | 0.2 % Show Material materials with Molybdenum of 0.2 % |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % |
Niobium | 0.15 - 0.45 % Show Material materials with Niobium of 0.15 - 0.45 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.5 % Show Material materials with Silicon of 0.5 % |
Sulfur | 0.03 % Show Material materials with Sulfur of 0.03 % |