Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 18 % Show Material materials with Elongation A50 of 18 % |
Hardness, Brinell | 20.0 °C | 163 - 217 [-] Show Material materials with Hardness, Brinell of 163 - 217 [-] |
Reduction of area | 20.0 °C | 45 % Show Material materials with Reduction of area of 45 % |
Tensile strength | 20.0 °C | 550 MPa Show Material materials with Tensile strength of 550 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 310 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 310 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.38 - 0.48 % Show Material materials with Carbon of 0.38 - 0.48 % |
Chromium | 0.8 - 1.2 % Show Material materials with Chromium of 0.8 - 1.2 % |
Manganese | 0.75 - 1.1 % Show Material materials with Manganese of 0.75 - 1.1 % |
Molybdenum | 0.15 - 0.25 % Show Material materials with Molybdenum of 0.15 - 0.25 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.15 - 0.4 % Show Material materials with Silicon of 0.15 - 0.4 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |
Vanadium | 0.1 % Show Material materials with Vanadium of 0.1 % |