General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 20.0 °C | 7.9 - 8.2 g/cm³ Show Material materials with Density of 7.9 - 8.2 g/cm³ | Typical for Austenitic Stainless Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 195 GPa Show Material materials with Elastic modulus of 195 GPa | Typical for Austenitic Stainless Steel |
Elongation A50 | 20.0 °C | 18 % Show Material materials with Elongation A50 of 18 % | |
Hardness, Brinell | 20.0 °C | 163 - 217 [-] Show Material materials with Hardness, Brinell of 163 - 217 [-] | |
Poisson's ratio | 20.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Austenitic Stainless Steel |
Reduction of area | 20.0 °C | 45 % Show Material materials with Reduction of area of 45 % | |
Tensile strength | 20.0 °C | 550 MPa Show Material materials with Tensile strength of 550 MPa | |
Yield Strength Rp0.2, short transverse | 20.0 °C | 310 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 310 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 20.0 °C | 1.7E-5 - 1.9E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K | Typical for Austenitic Stainless Steel |
Melting point | 1375 - 1450 °C Show Material materials with Melting point of 1375 - 1450 °C | Typical for Austenitic Stainless Steel | |
Specific heat capacity | 20.0 °C | 440 J/(kg·K) Show Material materials with Specific heat capacity of 440 J/(kg·K) | Typical for Austenitic Stainless Steel |
Thermal conductivity | 20.0 °C | 11 - 21 W/(m·K) Show Material materials with Thermal conductivity of 11 - 21 W/(m·K) | Typical for Austenitic Stainless Steel |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 20.0 °C | 8.5E-7 Ω·m Show Material materials with Electrical resistivity of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.3 - 0.35 % Show Material materials with Carbon of 0.3 - 0.35 % |
Chromium | 1 - 1.4 % Show Material materials with Chromium of 1 - 1.4 % |
Manganese | 0.4 - 0.8 % Show Material materials with Manganese of 0.4 - 0.8 % |
Molybdenum | 0.2 - 0.35 % Show Material materials with Molybdenum of 0.2 - 0.35 % |
Nickel | 1.3 - 1.7 % Show Material materials with Nickel of 1.3 - 1.7 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.15 - 0.4 % Show Material materials with Silicon of 0.15 - 0.4 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |
Vanadium | 0.15 % Show Material materials with Vanadium of 0.15 % |