General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation A50 | 23.0 °C | 20 % Show Material materials with Elongation A50 of 20 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Tensile strength | 23.0 °C | 310 MPa Show Material materials with Tensile strength of 310 MPa | |
Yield strength | 23.0 °C | 230 MPa Show Material materials with Yield strength of 230 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.2 % Show Material materials with Carbon of 0.2 % |
Chromium | 0.15 % Show Material materials with Chromium of 0.15 % |
Copper | 0.25 % Show Material materials with Copper of 0.25 % |
Manganese | 1.35 % Show Material materials with Manganese of 1.35 % |
Molybdenum | 0.06 % Show Material materials with Molybdenum of 0.06 % |
Nickel | 0.2 % Show Material materials with Nickel of 0.2 % |
Niobium | 8E-3 % Show Material materials with Niobium of 8E-3 % |
Phosphorus | 0.04 % Show Material materials with Phosphorus of 0.04 % |
Sulfur | 0.04 % Show Material materials with Sulfur of 0.04 % |
Titanium | 0.03 % Show Material materials with Titanium of 0.03 % |
Vanadium | 8E-3 % Show Material materials with Vanadium of 8E-3 % |