General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 8.8 g/cm³ Show Material materials with Density of 8.8 g/cm³ | Typical for Nickel Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Nickel Steel |
Elongation A50 | 23.0 °C | 38 % Show Material materials with Elongation A50 of 38 % | |
Hardness, Rockwell Superficial 15-T | 23.0 °C | 82 [-] Show Material materials with Hardness, Rockwell Superficial 15-T of 82 [-] | |
Hardness, Vickers | 23.0 °C | 130 [-] Show Material materials with Hardness, Vickers of 130 [-] | |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Nickel Steel |
Shear modulus | 23.0 °C | 76 GPa Show Material materials with Shear modulus of 76 GPa | Typical for Nickel Steel |
Tensile strength | 23.0 °C | 500 MPa Show Material materials with Tensile strength of 500 MPa | |
Yield strength Rp0.2 | 23.0 °C | 220 MPa Show Material materials with Yield strength Rp0.2 of 220 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Melting point | 1316 - 1595 °C Show Material materials with Melting point of 1316 - 1595 °C | Typical for Nickel Steel | |
Specific heat capacity | 23.0 °C | 456 J/(kg·K) Show Material materials with Specific heat capacity of 456 J/(kg·K) | Typical for Nickel Steel |
Thermal conductivity | 23.0 °C | 10 - 50 W/(m·K) Show Material materials with Thermal conductivity of 10 - 50 W/(m·K) | Typical for Nickel Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.05 % Show Material materials with Carbon of 0.05 % |
Chromium | 0.3 % Show Material materials with Chromium of 0.3 % |
Cobalt | 0.5 % Show Material materials with Cobalt of 0.5 % |
Copper | 0.3 % Show Material materials with Copper of 0.3 % |
Manganese | 0.8 % Show Material materials with Manganese of 0.8 % |
Molybdenum | 0.3 % Show Material materials with Molybdenum of 0.3 % |
Nickel | 43.5 - 46.5 % Show Material materials with Nickel of 43.5 - 46.5 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.5 % Show Material materials with Silicon of 0.5 % |
Sulfur | 0.01 % Show Material materials with Sulfur of 0.01 % |