Mechanical

PropertyTemperatureValue

Elongation A50

23.0 °C

16.5 - 30 %

Show Material materials with Elongation A50 of 16.5 - 30 %

Tensile strength

23.0 °C

485 MPa

Show Material materials with Tensile strength of 485 MPa

Yield strength

23.0 °C

275 MPa

Show Material materials with Yield strength of 275 MPa

Chemical properties

PropertyValue

Carbon

0.35 %

Show Material materials with Carbon of 0.35 %

Chromium

0.4 %

Show Material materials with Chromium of 0.4 %

Copper

0.4 %

Show Material materials with Copper of 0.4 %

Manganese

0.29 - 1.06 %

Show Material materials with Manganese of 0.29 - 1.06 %

Molybdenum

0.15 %

Show Material materials with Molybdenum of 0.15 %

Nickel

0.4 %

Show Material materials with Nickel of 0.4 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

0.1 %

Show Material materials with Silicon of 0.1 %

Sulfur

0.035 %

Show Material materials with Sulfur of 0.035 %

Vanadium

0.08 %

Show Material materials with Vanadium of 0.08 %