Mechanical

PropertyTemperatureValue

Hardness, Brinell

23.0 °C

121 [-]

Show Material materials with Hardness, Brinell of 121 [-]

Hardness, Rockwell B

23.0 °C

70 [-]

Show Material materials with Hardness, Rockwell B of 70 [-]

Chemical properties

PropertyValue

Carbon

0.15 %

Show Material materials with Carbon of 0.15 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

0.4 %

Show Material materials with Silicon of 0.4 %

Sulfur

0.05 %

Show Material materials with Sulfur of 0.05 %